LOCTITE ABLESTIK 2035SC

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Loctite Ablestik 2035SC

Main features

  • Low cure temperature
  • Smart card applications
  • Fast cure

Product Description

LOCTITE® ABLESTIK 2035SC non-conductive die attach adhesive has been formulated for use in high throughput die attach applications. This material is designed to minimise stress and resulting warpage between dissimilar surfaces.

LOCTITE® ABLESTIK 2035SC is isothermal and based on a proprietary hybrid chemistry that offers low stress and cures  fast in relatively low temperatures. This combination makes it ideal for snap cure smart card applications.

 

Cure Schedule

  • 90 seconds @ 110°C
  • 60 seconds @ 120°C or 10 seconds @ 150°C
Product Family

ABLESTIK 2035SC

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 15 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
24 hours
Physical Properties
Thixotropic index
4.2
Viscosity
11,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity
0.35 W/m.K
Weight Loss @ 300°C
2.51 %

Additional Information

LOCTITE ABLESTIK 2035SC is isothermal at 80°C.

The following DSC graph shows 9.9mg on a 40°C/min ramp from 40-80°C with 15min dwell.