ABchimie AVR80 XY Removable Acrylic Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie AVR80 XY Removable Acrylic Coating

Main features

  • Excellent dielectric properties
  • Wide operating temperature range (-65°C to +150°C)
  • Removable

Product Description

ABchimie AVR80 XY is a flexible, transparent acrylic conformal coating designed to provide high‑performance protection for electronic assemblies operating in demanding environments. Formulated to meet stringent resistance and inspection requirements, AVR80 XY ensures long‑term reliability of sensitive circuitry. The coating can be completely removed using ABchimie SND (100% ozone‑friendly) or DNS removers.

Product Key Features

  • Excellent adhesion in all climatic conditions
  • Resistant to mould growth
  • Wide operating temperature range: –65°C to +150°C
  • Can be soldered through without generating toxic gases
  • Halogen-free formulation

Applications

  • Protection of printed circuit boards (PCBs) in harsh environments
  • Electronics exposed to thermal cycling, moisture, or chemical stress

Qualifications

  • L QMJU2 approval (File E308681)
  • Meets IPC‑CC‑830 requirements
  • Certified to NF EN 61086‑2, NF EN 45545, NF EN 16101, and NF EN 16102
Product Family

ABCHIMIE AVR80XY

1. Select Package Type
2. Select Version
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pale liquid
Electrical Properties
Breakdown Voltage
1500 V
Dielectric Strength
50 kV/mm
Dissipation Factor @ 25°C /1000 kHz
0.01
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
130 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
280 ppm/°C
Flash Point
25 °C
Glass Transition Temperature (Tg)
29 °C
Operating Temperature
-65 - +150 °C
UL 94 Rating
V-0

Additional Information

Frequently Asked Questions About ABchimie® AVR80 XY

What makes AVR80 XY suitable for high-spec industries?


AVR80 XY is formulated to meet the most stringent resistance requirements. It holds UL QMJU2 (File E308681), NF EN 61086-2, and railway fire/smoke approvals (NF EN 45545, 16101, 16102). It is specifically engineered for environments requiring elite protection against moisture and contaminants.

How is AVR80 XY removed or repaired?

Despite its high resistance, AVR80 XY remains a flexible acrylic that is fully removable with ABchimie SND. It can also be safely soldered through for component replacement without the release of toxic isocyanate gases.

ABchimie® AVR80 XY: Elite Circuit Protection


ABchimie® AVR80 XY is a flexible, Halogen-free transparent acrylic coating designed for electronic circuitry in extreme conditions. It offers excellent dielectric properties and a wide operating temperature range from -65°C to +150°C, ensuring stability where standard coatings might fail.

Key Features & Benefits

Universal Adhesion

Exceptional bonding under all climatic conditions. Its resistance to mould growth makes it ideal for tropical and high-humidity applications.

Inspection Ready

Contains a built-in UV fluorescing tracer to facilitate rapid inspection of coverage and uniformity under blacklight.


Product Selector Guide

Property AVR80 AVR80 BA AVR80R AVR80 XY
Type Standard Non-Toxic High Solid High-Spec Flex
Thinner DVA DVA BA DVA / DVA-R DVA-XY
Best For General Use Eco-Fast High Solids Railway/Military

Instructions for Use

AVR80 XY can be applied via spraying, dipping, or brushing. To ensure full environmental protection, a minimum dry film thickness of 25 microns is recommended. Application is most effective when workshop temperatures are above 16°C and relative humidity is below 75%.

Moisture Management & Application

All PCBs, being composite materials, naturally absorb moisture. If this is not removed, the conformal coating may not protect to its fullest extent.

  • Pre-Drying: We recommend oven drying (3-4 hours at 60°C) or vacuum desiccation prior to coating to ensure maximum adhesion and reliability.
  • Repairability: Rework can be performed by soldering directly through the coating or by total removal using ABchimie SND or DNS.
  • Inspection: Use UV light after application; stronger reflected light indicates a thicker coating layer, allowing for precise quality control.