ABchimie AVR80 BA Non-Toxic Acrylic Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie AVR80 BA Non-Toxic Acrylic Coating

Main features

  • Fluoresces under UV light
  • Excellent adhesion
  • Halogen‑free formulation

Product Description

ABchimie AVR80 BA is a non‑toxic, flexible, transparent acrylic conformal coating designed to deliver high‑performance protection for electronic circuitry in demanding environments. This environmentally friendly formulation provides exceptional resistance to moisture, chemicals, and thermal stress. AVR80 BA can be completely removed using ABchimie SND or ABclean (100% ozone‑friendly), ensuring easy rework and maintenance.

A low‑viscosity, ready‑to‑use version (AVR80 BA DS) is also available for applications requiring excellent flow and penetration.

Product Key Features

  • Excellent adhesion under all climatic and environmental conditions
  • Resistant to mould and biological growth
  • Wide operating temperature range: –65°C to +150°C
  • Halogen‑free formulation

Applications

Qualifications

  • UL94 V‑0 approval (File E308681)
  • Meets IPC‑CC‑830 and MIL‑I‑46058C conformal coating standards
  • Certified to NF EN 61086‑2, NF EN 45545, NF EN 16101, and NF EN 16102
Product Family

ABCHIMIE AVR80BA

1. Select Package Type
2. Select Version
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pale liquid
Specific Gravity
0.93
Electrical Properties
Breakdown Voltage
1500 V
Dielectric Strength
50 kV/mm
Dissipation Factor @ 25°C /1000 kHz
0.01
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
130 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
280 ppm/°C
Glass Transition Temperature (Tg)
29 °C
Operating Temperature
-65 - +150 °C
UL 94 Rating
V-0

Additional Information

Frequently Asked Questions About ABchimie® AVR80 BA

What makes AVR80 BA "Non-Toxic"?


AVR80 BA is formulated without hazardous solvents like Toluene or Xylene. This makes it a safer choice for operators while maintaining compliance with UL94V0 and MIL-I-46058C. It provides the same high-level protection as standard acrylics without the associated toxicity.

Is there a ready-to-use version available?

Yes. For applications requiring a lower viscosity without manual thinning, AVR80 BA DS is available. It is a ready-to-use version designed for rapid integration into spray or dip coating lines.

ABchimie® AVR80 BA: Safe, High-Spec Protection


ABchimie® AVR80 BA is a flexible, Halogen-free, and non-toxic transparent acrylic coating. It is specifically engineered to meet the highest resistance requirements (including NF EN 45545 for rail safety) while ensuring a safer manufacturing environment through its isocyanate-free formulation.

Performance Features

Environmental Reliability

Maintains excellent adhesion and dielectric properties under extreme climatic conditions, with an operating range from -65°C to +150°C.

Rework Friendly

Can be safely soldered through for repairs or fully removed using ABchimie SND or ABclean. It is also resistant to mould growth.


Product Selector Guide

Property AVR80 BA AVR80 BA HV AVR80 BA DS
Form Non-Toxic Liquid High Viscosity Gel Low Viscosity (Ready to Use)
Drying 10-20 min (Touch) <30 min (Touch) Very Fast drying
Method Spray/Dip/Brush Dispense/Brush Automated Spray/Dip

Instructions for Use

AVR80 BA is suitable for spraying, dipping, or brushing. Standard application typically targets a dry film thickness of 25 microns. Optimal results are achieved at workshop temperatures above 16°C with relative humidity below 75%.

Process Recommendations

  • Moisture Control: PCBs are composite materials that absorb moisture. To ensure full protection, remove moisture via an oven bake (3-4 hours at 60°C) before coating.
  • UV Inspection: The integrated UV tracer glows under blacklight. The brighter the reflection, the thicker the coating layer, allowing for simple and effective quality control.
  • Homogenization: Always mix before use. If you observe a "white veil" or cloudiness, simply stir the varnish to restore a homogeneous consistency.
  • Immediate Coating: Boards can be coated immediately after soldering. If boards have been stored for over 48 hours, a drying cycle is required.
Contact Us →

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers