ABchimie AVR80 Removable Acrylic Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie AVR80 Removable Acrylic Coating

Main features

  • Halogen-free
  • Excellent adhesion
  • Fluoresces under UV light

Product Description

ABchimie AVR80 is a flexible, transparent acrylic conformal coating formulated to deliver high‑performance protection for electronic circuitry operating in demanding environments. Engineered for excellent resistance to moisture, chemicals, and thermal stress, AVR80 ensures long‑term reliability of sensitive electronic assemblies. It is fully removable using ABchimie SND or ABclean (100% ozone‑friendly solutions)

Product Key Features

  • Excellent adhesion across a wide range of climatic conditions
  • Wide operating temperature range: –65°C to +150°C
  • Resistant to mould and biological growth
  • Halogen‑free formulation

Applications

Qualifications

  • UL94 V‑0 approval (File E308681)
  • Meets IPC‑CC‑830 and MIL‑I‑46058C requirements
  • Certified to NF EN 61086‑2, NF EN 45545, NF EN 16101, and NF EN 16102
Product Family

ABCHIMIE AVR80

1. Select Package Type
2. Select Version
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pale liquid
Specific Gravity
0.93
Electrical Properties
Breakdown Voltage
1500 V
Dielectric Strength
50 kV/mm
Dissipation Factor @ 25°C /1000 kHz
0.01
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
130 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
280 ppm/°C
Glass Transition Temperature (Tg)
29 °C
Operating Temperature
-65 - +150 °C
UL 94 Rating
V-0

Additional Information

Frequently Asked Questions About ABchimie® AVR80

Which standards does ABchimie® AVR80 meet?


AVR80 is formulated for the highest resistance requirements. It is UL94V0 approved (File E308681) and meets MIL-I-46058C and IPC-CC-830. Additionally, it holds NF EN 61086-2 and fire/smoke approvals (NF EN 45545, 16101, 16102), making it suitable for railway and aerospace applications.

Can I solder through the coating for repairs?

Yes. One of the standout features of AVR80 is that it can be soldered through without the risk of producing highly toxic gases, such as isocyanates. For full removal, it is compatible with ABchimie SND or ABclean (100% Ozone Friendly).

ABchimie® AVR80 High-Spec Acrylic Coating


ABchimie® AVR80 is a flexible, transparent, and Halogen-free acrylic coating. Engineered for elite protection of electronic circuitry, it offers excellent adhesion under all climatic conditions and remains stable across a wide temperature range of -65°C to +150°C.

Performance Features

Safety & Compliance

Certified UL94V0 and NF EN 45545. Formulated without isocyanates, ensuring a safer work environment during application and rework.

Climatic & Bio-Resistance

Specifically designed to resist mould growth and maintain superior dielectric properties in high-humidity or tropical climates.


Product Selector Guide

Property AVR80 (Standard) AVR80 BA (Non-Toxic) AVR80R (High Solid)
Key Feature Universal High-Spec Toluene/Xylene Free 60% Solids / Repairable
Approvals UL94V0, MIL, IPC, NF EN UL94V0, IPC-CC-830 UL94V0, MIL-I-46058C
Solvent Removal ABchimie SND / ABclean (Ozone Friendly)

Instructions for Use

AVR80 can be applied through spraying, dipping, or brushing. For volume production, automated spraying or dipping is recommended to ensure a consistent 25-micron dry film thickness.

Optimal Application Protocol

  • Pre-Cleaning: PCBAs should be clean and dry. A pre-bake in an oven (3-4 hours at 60°C) is recommended to remove absorbed moisture from composite substrates.
  • Rework: If rework is required, you can safely solder through the coating. The absence of isocyanates prevents the release of highly toxic fumes during the heating process.
  • Homogenization: If a "white veil" or cloudiness is observed in the liquid, stir/mix the varnish to restore a homogeneous state before application.
  • UV Inspection: Use blacklight (UV light) to inspect the board; the coating's fluorescence makes it easy to spot uncoated areas or uneven applications.