ABchimie746E UV LED Soft UV Cure Conformal Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie746E UV LED Soft UV Cure Conformal Coating

Main features

  • Excellent adhesion
  • UV‑fluorescent for easy inspection
  • Certified UL94 V‑0 and UL746E

Product Description

ABchimie 746E UV LED is a transparent, single‑component, LED‑curable conformal coating engineered to protect PCBs exposed to harsh environments. It features dual‑cure technology (UV LED + humidity) for complete crosslinking, including areas shadowed from UV LED exposure.

Its optimized formulation cures rapidly under UV LED light sources, enabling energy‑efficient, low‑temperature, high‑speed manufacturing. With low viscosity designed for precise application around 80 µm, ABchimie 746E UV LED is ideal for advanced selective coating processes.

Product Key Features

  • Excellent adhesion in harsh climatic and environmental conditions
  • UV‑fluorescent for easy inspection of coating uniformity
  • Operating temperature range: –65°C to +150°C
  • Safe solder‑through performance without toxic gas formation
  • Certified UL94 V‑0 and UL746E (QMJU2‑E308681)

Applications

  • High‑volume production lines requiring instant UV LED curing
  • Complex assemblies with shadowed areas requiring dual‑cure reliability
Product Family

ABCHIMIE 746EUVLED

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent yellow liquid
Film Thickness
30 - 150 µm
Physical Properties
Viscosity
0.05 - 0.1 mPa.s
Electrical Properties
Breakdown Voltage
1750 V
Dielectric Strength
60 kV/mm
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
200 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
250 ppm/°C
Glass Transition Temperature (Tg)
12.5 °C
Operating Temperature
-65 - +150 °C
UL 94 Rating
V-0

Additional Information

Frequently Asked Questions About ABChimie® 746E UV LED

What are typical applications for ABChimie® 746E UV LED?

ABChimie® 746E UV LED is a low viscosity UV-curable conformal coating designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:

  • Automotive electronics (e.g., control units, sensors)
  • Industrial automation (e.g., motor drives, PLCs)
  • Consumer electronics (e.g., smart devices, wearables)
  • Other high-reliability electronic assemblies

Why choose ABChimie® 746E UV LED?

ABChimie® 746E UV LED delivers rapid UV curing, excellent electrical insulation, optical transparency, and strong adhesion to flexible substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.

What is the shelf life of ABChimie® 746E UV LED?

ABChimie® 746E UV LED has a shelf life of 12 months when stored at 5–30°C in tightly sealed containers. Prior to use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance.

What happens after the shelf life?

Using ABChimie® 746E UV LED past its shelf life may alter viscosity, affecting uniformity and application performance. Always use an in-date product for reliable results.

What is the recommended thickness for ABChimie® 746E UV LED?

ABChimie® 746E UV LED coating thickness depends on the application method.

Recommended thickness 40–120 microns
Spraying (two crossed layers): 60–80 microns
Brushing: 40-60 microns
Selective coating machine (film coater): 80–120 microns

What safety precautions should I take?

Use ABChimie® 746E UV LED in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.

Can I adjust the viscosity?

ABChimie® 746E UV LED can be customized for variable viscosities. Contact our team for guidance.

Should I control the application environment?

ABChimie® 746E UV LED should be applied at a minimum temperature of 16°C and a minimum relative humidity of 50%. The relative humidity of at least 50% is recommended for the secondary polymerization. Before applying, the PCB must be clean, dry, and free of moisture. A stage in an oven at 80°C for 4 hours is usually sufficient.

Learn More About ABChimie® 746E UV LED

ABChimie® 746E UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable conformal coating delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for automotive, industrial, consumer, and high-reliability assemblies. It also contains a UV tracer for easy inspection.

Main Advantages of ABChimie 746E UV LED

dual cure technology

ABChimie® 746E UV LED cures through a dual mechanism: UV exposure initiates rapid surface curing, while moisture ensures complete curing throughout the coating.

mechanical protection

Provides excellent mechanical protection, resisting scratches, abrasion, and minor impacts to ensure long-term component stability.

ability to solder

Can be soldered through without generating highly toxic gases, maintaining coating integrity.

excellent adhesion in harsh environments

Provides strong adhesion in harsh conditions, resisting moisture, chemicals, and temperature changes.


How to Choose a Conformal Coating

  • ✔ Norms & Compliance
  • ✔ Environment / Exposure Conditions
  • ✔ Repairability
  • ✔ Electrical Performance
  • ✔ Application Method
  • ✔ Operating Temperature

Compliance You Can Trust ✅

  • REACH Compliant
  • RoHS 2011/65/EU Compliant
    UL94 V0
    UL746E (QMJU2-E308681)

Curing Tip: ABChimie 746E UV LED cures with UV rays. Use the recommended equipment and settings to achieve optimal properties.

Ref. Leistung / ref power ln % over wavelength in nm

PTM6000HV-SP thermal impedance versus bondline thickness

Key Curing Properties

Lamp Type
LED
Emission Spectrum of LED
395 nm
Minimum UVA Dose
3000 mJ/cm2
Coating Thickness
100 μm
Minimum UVA Power
500 mW/cm2

Typical property values shown for reference only and should not be used as specifications.

Application tips

How to Optimise for the Best Results

 
PCB Preparation

PCBs must be completely dry and thoroughly clean, with no dust, grease, wax, or other contaminants. All flux residues must be removed to prevent corrosion or malfunctions.

How to clean the PCB

For cleaning equipment or removing uncured ABChimie 746E UV or UV LED varnish, use SND or ABclean solvent.

UV Recommendation

Use the correct UV equipment and recommended settings to achieve optimal properties. UV exposure plus moisture curing ensures complete polymerization.

Curing Mechanism

Curing Mechanism: UV light creates the first cure, and after 7 days, the moisture from the environment completes the curing process.

Double-Curing Mechanism

How does Moisture Cure Work?

During UV curing, exposure to UV light activates the photoinitiators in the conformal coating, triggering rapid polymerization of the resin. This results in an immediate surface cure and fast development of handling strength. UV curing provides precise, on-demand curing in exposed areas, enabling high-throughput processing while maintaining coating uniformity.

ABChimie 746E UV and ABChimie 746E UV LED use the same dual curing mechanism to ensure complete curing, including in shadowed or hard-to-reach areas. Initial curing is achieved by UV exposure, while a secondary moisture-activated cure completes the process at ambient temperature. For full curing in shaded areas, a minimum relative humidity of 50% is required for at least 7 days.

ABChimie 746E UV LED is also available in the mercury lamp version, which cures with a mercury lamp.

ABChimie 746E UV [Go to 746E UV Product Page↗]

  • Conformal Coating
  • Fluorescent under UV light
  • Excellent adhesion to flexible substrates
  • Dual curing with UV light exposure and moisture curing

Best suited for: High-speed process using LED light for curing

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers