3M TE031

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M TE031

Main features

  • 30-Second Handling Strength
  • Two-Minute Assembly Window
  • Flexible Plastic Bonding

Product Description

3M Scotch-Weld PUR Adhesive TE031 is a one-part, warm-applied polyurethane reactive adhesive for fast plastic assembly. The 100% solids material is applied at 121 deg C, provides a typical two-minute open time, and reaches handling strength in about 30 seconds under the stated test definition. Moisture cure builds a flexible bond, with strong peel results on polystyrene, acrylic, polycarbonate, PVC, and fiber-reinforced plastic. Moisture must reach the bondline: do not use TE031 for metal-to-metal, glass-to-glass, or metal-to-glass joints, and avoid untreated polyolefins. The extrudable format is suitable for cartridge or bulk PUR dispensing equipment.

Key features

  • Fast handling strength: Reaches the stated 34 kPa handling-strength threshold in about 30 seconds at room temperature.
  • Two-minute assembly window: Provides a defined open time for joining and fixing parts after warm application.
  • Flexible plastic bonding: A typical 725% cured elongation allows the adhesive layer to deform before breaking.

Applications

Applications include bonding polystyrene, acrylic, polycarbonate, PVC, wood, and fiber-reinforced plastic where moisture reaches the bondline; exclude untreated polyolefins and metal-to-metal, glass-to-glass, or metal-to-glass joints.

Product Family

3M TE031

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White/Off-White
Density (g)
1.04 g/cm3
Physical Properties
Viscosity
at 121 °C (250 °F): 13,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Open and handling times are typical and vary with adhesive temperature and application conditions.

PropertyValueUnitMethod / condition
ColorWhite to off-whiteSolid state
Viscosity13,000cP121 deg C; Brookfield Thermosel, spindle 27
Molten density1.04g/cm^3Typical
Open time2minutes3.2 mm bead on a non-metallic surface; room-temperature environment
Time to handling strength30secondsTime to support a 34 kPa tensile load; room-temperature environment
Application temperature121deg CWarm-applied adhesive
Technical properties

After-processing / final-state properties

Mechanical and peel values are typical for the stated specimens, dwell, temperature, and test configuration.

PropertyValueUnitMethod / condition
Shore D hardness50ASTM D2240; cured material at 23 deg C
Modulus39MPaASTM D638 / ISO 527; 7 d at 23 deg C; 0.3 to 0.4 mm film
Elongation at break725%ASTM D638 / ISO 527; 7 d at 23 deg C; 0.3 to 0.4 mm film
Tensile strength at break27MPaASTM D638 / ISO 527; 7 d at 23 deg C; 0.3 to 0.4 mm film
180 deg peel adhesion114N/cmPolystyrene; 168 h dwell at 25 deg C; 51 mm/min
180 deg peel adhesion135N/cmAcrylic; 168 h dwell at 25 deg C; 51 mm/min

Leading Brands Trust in Our Products and Services