3M TC-2707

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M TC-2707

Main features

  • Thermally Conductive Bonding
  • 60-Minute Working Window
  • Low-Viscosity Gap Filling

Product Description

3M Thermally Conductive Epoxy Adhesive TC-2707 is a two-part aluminum-filled epoxy adhesive that creates thermally conductive bonds in electronic and thermal-management assemblies. The 2:1 by-volume mix has a typical 60-minute work life at 23 deg C and a mixed viscosity of 60,000 cP for gap filling, potting, and thin bondlines. Typical cured thermal conductivity is 0.72 W/(m K), with ambient and heat-cure schedules available. The aluminum filler can create an electrical bridge if it is trapped between energized surfaces, so TC-2707 is not intended where reliable electrical insulation or powered-circuit isolation is required.

Key features

  • Thermally conductive bonding: A typical 0.72 W/(m K) cured value combines heat transfer with adhesive attachment.
  • Controlled working window: A typical 60-minute work life at 23 deg C supports mixing, placement, and assembly.
  • Gap-fill and potting flow: Mixed viscosity supports potting, general gap filling, and thin bondline application.

Applications

Applications include LED assembly, thermal fixing of battery cells, EV and HEV battery thermal management, potting, and general gap filling.

Product Family

3M TC-2707

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part A)
Base: 95000 mPa.s
Viscosity (Part B)
Accelerator: 25000 mPa.s
General Properties
Component System
A: Epoxy | B: Amine
Filler Content
Aluminum: 50% %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the accelerator or mixed system as identified.

PropertyValueUnitMethod / condition
Accelerator viscosity25,000cP40 mm, 2 deg cone at 10 s^-1
Mixed viscosity60,000cP40 mm, 2 deg cone at 10 s^-1
Aluminum filler content50wt%As supplied
Mix ratio, B:A2:1by volumeTwo-part system
Work life60minutes23 deg C
Technical properties

After-processing / final-state properties

Cured values are typical; TC-2707 is not intended where reliable electrical insulation is required.

PropertyValueUnitMethod / condition
Shore D hardness80ASTM D2240
Thermal conductivity0.72W/(m K)ASTM D5470; cured material
Volume resistivity1.6 x 10^11ohm cmASTM D257; aluminum filler can lower effective values when pinched
Overlap shear strength>18.62N/mm^2ASTM D1002; 23 deg C/24 h, 90 deg C/30 min, or 120 deg C/10 min cure
T-peel strength>7lb/in widthASTM D1876; same three cure schedules

Leading Brands Trust in Our Products and Services