3M SJ5816

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M SJ5816

Main features

  • Die-Cut Protective Conversion
  • Skid-Resistant Polyurethane Cushioning
  • High-Tack PSA Installation

Product Description

3M Bumpon Resilient Rollstock SJ5816 is a black, self-adhesive solid polyurethane rollstock for conversion into die-cut feet, stops, spacers, and cushioning parts. The 1.6 mm sheet combines Shore M 72 polyurethane with an R-30 natural-rubber pressure-sensitive adhesive and PET release liner. Its resilient, skid-resistant surface is used to reduce vibration and noise, cushion components, and protect finished surfaces from scratching or marring. The roll format supports custom shapes and sizes, while the pressure-sensitive backing simplifies placement after die cutting. SJ5816 is intended primarily for interior applications; protected outdoor use may show discoloration or chalking.

Key features

  • Die-cut rollstock conversion: Converts into custom feet, stops, spacers, gaskets, and protective shapes.
  • Skid-resistant cushioning: Solid polyurethane provides grip, cushioning, and vibration or noise damping in compact assemblies.
  • Natural-rubber PSA mounting: R-30 adhesive provides high initial tack for pressure-sensitive placement after conversion.

Applications

Applications include die-cut protective feet, stops, spacers, gaskets, anti-rattle parts, cushioning elements, and non-scratch surface protection.

Product Family

3M SJ5816

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
natural rubber (R-30)
Density (g)
1.3 g/cm3
Release Liner
4 mil, silicone coated PET
Mechanical Properties
Elongation
100 %
Thermal Properties
UL 94 Rating
HB
Electrical Properties
Dielectric Strength
7.87 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Construction and physical values apply to SJ5816 or the SJ5800 series as indicated.

PropertyValueUnitMethod / condition
ColorBlackSJ5816
ElastomerSolid polyurethaneSJ5800 series construction
AdhesiveR-30 natural rubberPressure-sensitive adhesive
Surface finishMattePolyurethane surface
Nominal thickness1.6mmASTM D3767 Procedure A; measured without liner
Hardness72Shore MASTM D2240
Technical properties

After-processing / final-state properties

Performance values are typical for SJ5816 or the SJ5800 series under the stated test conditions.

PropertyValueUnitMethod / condition
Kinetic coefficient of friction>1ASTM D1894; stainless steel and glass
Kinetic coefficient of friction0.8 to 1.4ASTM D1894; Formica laminate and wood
90 deg peel adhesion25oz/0.5 inPolypropylene, polystyrene, or ABS; 72 h dwell; 3M TM-2011
90 deg peel adhesion22oz/0.5 inStainless steel or aluminum; 72 h dwell; 3M TM-2011
Recommended maximum load100psi21 to 49 deg C; SJ5800 series
Service temperature-34 to 66deg C107 deg C intermittent exposure

Leading Brands Trust in Our Products and Services