3M™ Dual Lock™ Resealable Snap Tape SJ3540

Harmonization Code : 3926909790 |

3M™ Dual Lock™ Resealable Snap Tape SJ3540

Main features

  • Black, interlocking mushroom-shaped heads (250 stem density per square inch)
  • Mates with Type 170, Type 250 or Type 400 stem densities
  • Strong fastener secures with an audible snap, verifying closure

Product Description

3M™ Dual Lock™ Reclosable Fasteners SJ3540 is a high-performance reclosable fastening system designed with a synthetic rubber-based adhesive on the back of a durable black polypropylene strip. Featuring interlocking mushroom-shaped stems, these fasteners provide strong, reliable attachment with the ability to open and close repeatedly. They are engineered for bonding to a wide range of substrates, including low surface energy materials.

Product Key Features

  • Mushroom-shaped stems interlock securely for strong fastening with repeated opening and closing
  • Available in 250 stems per square inch for varying strength and engagement levels
  • Provides excellent initial tack, especially on low surface energy surfaces
  • Polypropylene backing ensures long-lasting performance
  • Can replace traditional fasteners such as screws, bolts, or snaps in many applications
  • Pressure-sensitive adhesive allows quick installation without special tools

Applications

  • Attaching panels, covers, and access doors
  • Mounting lightweight components and assemblies
  • Securing signage, displays, and decorative elements
  • Applications requiring frequent removal and reattachment
  • Bonding to plastics and other low surface energy materials
  • General industrial and commercial fastening solutions
Product Family

3M SJ3540

1. Select Width
2. Select Length
3. Select Thickness
4. Select Color
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 2 weeks
Packaging
Please select Width, Length, Thickness and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Synthetic rubber