3M RP2110

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M RP2110

Main features

  • Aircraft Erosion-Protection Repair
  • Controlled 1:1 Cartridge Dispensing
  • Ten-Minute Working Window

Product Description

3M Scotch-Weld Repair Paste 2110 is a two-part, 100% solids urethane paste for repairing polyurethane erosion-protection films and coatings. The components dispense from 1:1 Duo-Pak cartridge formats through a static mixer with the 3M EPX applicator. A typical 10-minute work life provides the repair window before the material advances toward cure. It becomes tack-free in about six hours and reaches full cure in 24 hours at 25 deg C. The cured material forms a black polyurethane elastomer with sand and rain erosion resistance, making it suitable for localized repair of compatible aircraft protection systems.

Key features

  • Erosion-protection repair: Cures to a black polyurethane elastomer for localized repair of compatible aircraft erosion-protection films and coatings.
  • Controlled 1:1 cartridge mixing: Duo-Pak cartridges dispense both components through a static mixer in the specified ratio.
  • Ten-minute working window: Provides a typical 10-minute work life before progressing to a 24-hour full cure at 25 deg C.

Applications

Applications include repair of polyurethane erosion-protection films and coatings on helicopter rotor blades, leading edges, engine components, and other aircraft erosion areas.

Product Family

3M RP2110

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (A / B)
Physical Properties
Tack-Free Time
360 minutes
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Component values are typical and remain separated by Part A and Part B.

PropertyValueUnitMethod / condition
Part A colorTransparentVisual
Part B colorBlackVisual
Part A density1.05g/mLASTM D1875
Part B density1.05g/mLASTM D1875
Part A viscosity200,000 to 250,000cPASTM D2556
Part B viscosity70,000 to 80,000cPASTM D2556
Mix ratio1:1by volumeDuo-Pak cartridge
Work life10minutes3M test method C-548
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorBlackVisual; cured material
Density1.05g/mLASTM D792; cured material
Time to full cure24hoursASTM D4440; 25 deg C
Shore A hardness70ASTM D2240
Taber abrasion0.020gASTM D4060
Tack-free time6hours3M test method C-3173
Adhesion to polyurethane20lb/inASTM D3330, Method A
Adhesion to epoxy glass-fiber composite12lb/inASTM D3330, Method A

Leading Brands Trust in Our Products and Services