3M EC-3901

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3901

Main features

  • Metal And Glass Surface Priming
  • Improved Metal Corrosion Protection
  • Clean Surface Oxidation Protection

Product Description

3M Scotch-Weld Structural Adhesive Primer EC-3901 is a red, one-component metal and glass primer for use before compatible 3M Scotch-Weld film and liquid structural adhesives. Its low-viscosity liquid wets prepared surfaces and is designed to improve adhesion while adding corrosion protection and resistance to environmental exposure on metal. The primer also protects cleaned surfaces from oxidation while bonding operations are scheduled. Use it in prepared metal and glass bonding processes where a dedicated primer layer is needed before the structural adhesive is applied.

Key features

  • Metal And Glass Adhesion Primer: The one-component liquid prepares compatible metal and glass for structural bonding.
  • Improved Metal Corrosion Protection: The primer adds protection against corrosion and environmental exposure on metal.
  • Cleaned Surface Protection: Primed surfaces remain protected from oxidation until bonding can be completed.

Applications

Prepared metal and glass surfaces before compatible 3M Scotch-Weld film and liquid structural adhesive application.

Product Family

3M EC-3901

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
red
Physical Properties
Net Weight
779 kg/m3
Viscosity
5 mPa.s
Thermal Properties
Flash Point
16 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Product typeOne-component primer-As supplied
ColorRed-As supplied
ViscosityLow-Liquid primer for wetting prepared surfaces