3M EC-3549

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3549

Main features

  • High Peel Structural Durability
  • Impact Resistant Urethane Bonding
  • Controlled Sag Resistant Placement

Product Description

3M Scotch-Weld Urethane Adhesive EC-3549 B/A is a two-part, sag-resistant urethane adhesive for tough structural bonds on many primed or painted metals, plastics, wood, and composites. The mixed material resists sagging in approximately 30 seconds, helping control bead placement on vertical and irregular joints. A 60 minute work life provides time for application, alignment, and adjustment before cure at room temperature or with heat. On etched aluminum, published overlap shear reaches 2000 psi at 24 deg C and 2500 psi at -40 deg C under the specified test configuration.

Key features

  • High Peel Structural Bonding: The tough polyurethane is formulated for durable bonds with high peel strength.
  • Impact Resistant Performance: The cured adhesive tolerates shocks and collisions in structural assemblies.
  • Sag Resistant Placement: The mixed material resists sagging in approximately 30 seconds for accurate application.

Applications

Bonding compatible primed or painted metals, plastics, wood, and composites in tough structural assemblies.

Product Family

3M EC-3549

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Brown
Mix Ratio
1:1
Pot Life
40 minutes
Mechanical Properties
Elongation
100 %
Electrical Properties
Dielectric Strength
18.5 kV/mm
Volume Resistivity
2.6 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Product typeTwo-part urethane-Before cure
Work life60minAt room temperature
Sag resistanceApproximately 30secAfter mixing
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Overlap shear strength2500psiEtched aluminum; tested at -40 deg C
Overlap shear strength2000psiEtched aluminum; tested at 24 deg C
Overlap shear strength300psiEtched aluminum; tested at 82 deg C
Overlap shear strength1200psiAbraded and solvent-wiped steel; tested at 24 deg C
Handling-strength time7daysAt room temperature

Leading Brands Trust in Our Products and Services