3M Scotch-Weld Epoxy Adhesive EC-1838 B/A is a green, controlled-flow structural epoxy for prepared metals, wood, and selected plastics. Mix Part B and Part A at 4:5 by volume or 1:1 by weight; the paste provides a 60 minute work life at 23 deg C and limits migration after placement. Handling strength develops in 6 to 10 hours at room temperature or 15 to 20 minutes at 65 deg C. The cured adhesive reaches Shore D 82 hardness, 2% to 3% elongation, and a 55 deg C glass transition temperature.

Key features

  • Controlled Flow Placement: The paste formulation limits migration after the adhesive is applied.
  • One Hour Work Life: A 60 minute processing window supports coating, alignment, and fixturing.
  • Durable Structural Epoxy: High shear strength and environmental resistance support prepared industrial joints.

Applications

Structural bonding of prepared metals, wood, selected plastics, and assemblies requiring controlled adhesive flow.

Product Family

3M EC-1838

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (Accelerator | Base)
Other Properties
Storage Temperature
16 - 27 °C
Thermal Properties
Glass Transition Temperature (Tg)
55 °C
Electrical Properties
Volume Resistivity
1.5 x 10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Mix ratio by volume4:5B:ATwo-part system
Mix ratio by weight1:1B:ATwo-part system
Base colorWhite-Before mixing
Accelerator colorGreen-Before mixing
Base viscosity70000 to 600000cPAt 27 deg C
Accelerator viscosity300000 to 1000000cPAt 27 deg C
Work life60min100 g mixed at 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorGreen-Cured
Hardness82Shore DASTM D2240 at 23 deg C
Elongation at break2 to 3%At 23 deg C
Tensile strength at break4290psiAt 23 deg C
Glass transition temperature55deg CDSC midpoint
Volume resistivity1.5 x 10^15ohm-cmASTM D257 at 23 deg C