3M EC-1357

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M EC-1357

Main features

  • Fast Interior Contact Assembly
  • Positioning Time Before Contact
  • Flexible Coating Method Selection

Product Description

3M Scotch-Weld Neoprene High Performance Contact Adhesive EC-1357 is a fast-acting neoprene contact adhesive for aircraft-interior assemblies using rubber, fabric, foam, metal, wood veneer, plastic laminate, or honeycomb. Apply it by spray, brush, or roller, then use the 10 to 20 minute open time to align parts before contact. Qualified canvas-to-steel peel strength reaches 42 lb/in width after five days at 24 deg C, while three-week birch overlap shear reaches 536 psi at 24 deg C and 199 psi at 82 deg C.

Key features

  • Rapid Contact Strength Build: The adhesive develops high initial strength for efficient assembly.
  • Positioning Time Before Contact: A 10 to 20 minute open time supports alignment and adjustment.
  • Spray Brush Or Roller Application: Multiple coating methods accommodate varied part sizes and shapes.

Applications

Aircraft-interior panels, wood veneer, rubber, fabric, foam, metal, plastic laminate, and compatible honeycomb assembly.

Technical Specifications

General Properties
Color
Gray/Green, Light Yellow
Solids
23 - 27 %
Thermal Properties
Flash Point
-26 °C
Physical Properties
Viscosity
200 - 450 mPa.s
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel strength42lb/in widthCanvas to steel after 5 days at 24 deg C
Overlap shear strength536psiBirch to birch after 3 weeks at 24 deg C
Low-temperature overlap shear strength964psiBirch to birch after 3 weeks; tested at -34 deg C
High-temperature overlap shear strength199psiBirch to birch after 3 weeks; tested at 82 deg C