3M™ Scotch-Weld™ Low Odor Acrylic Adhesive DP8810NS

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Scotch-Weld™ Low Odor Acrylic Adhesive DP8810NS

Main features

  • Toughened
  • Excellent shear strength
  • High peel and impact strength

Product Description

3M™ Scotch-Weld™ DP8810NS Low Odor Acrylic Adhesive is a high performance, two-part acrylic adhesive that offer excellent shear, peel, and impact performance. DP8810NS provides improved adhesion to many plastics and metals, including those with slightly oily surfaces. It also features a fast rate of strength build, providing structural strength in minutes. The low odor and non-flammability features also make them easier to incorporate into a manufacturing process.

DP8810NS Green has been tested for surface flammability, smoke, toxic gas generation, and caloric content per ASTM E162, ASTM E662, ASTM E1354, Bombardier SMP 800-C, and Boeing BSS 7239 test methods.

Product Key Features

  • Toughened
  • Excellent shear strength
  • High peel and impact strength
  • 10:1 mix ratio control bond line thickness
  • Variety of open times available
  • Increased cure speed with applied heat
  • Contain glass beads (0.010” diameter) to control bond line thickness

Applications

  • Bonding metals such as aluminum, steel, and stainless steel
  • Adhesion of plastics including ABS, acrylics, polycarbonate, and PVC
  • Assembly of transportation components (rail, bus, automotive, aerospace interiors)
  • Structural panel bonding and composite assembly
  • Signage, display, and general industrial fabrication
  • Bonding dissimilar materials where minimal surface preparation is preferred
  • Applications requiring fast fixturing and high impact resistance
Product Family

3M DP8810NS

1. Select Color
2. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 2 weeks
Packaging
Please select Color and Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Off-White/Blue
Density (g)
1.06 g/cm3
Mix Ratio
10:1
Work life @25°C
0.2 hours
Physical Properties
Viscosity
45,000 mPa.s