Main features

  • Flexible Dissimilar Material Bonding
  • Non Sag Bondline Control
  • Fast Handling Strength Development

Product Description

3M Scotch-Weld Flexible Acrylic Adhesive DP8610NS is a black, low-odor, non-flammable two-part acrylic structural adhesive with a 10:1 mix ratio. The non-sag formulation and internal spacer beads support controlled bondline placement on panels, frames, thin materials, and dissimilar substrates. A 7 minute work life and 20 minute handling-strength time support fast room-temperature assembly. After cure, the flexible adhesive provides 140% elongation and qualified overlap-shear performance across metals, plastics, and fiber-reinforced composites for efficient industrial panel assembly.

Key features

  • Flexible Dissimilar Material Bonding: The acrylic system bonds compatible metals, plastics, and composite panels.
  • Non Sag Bondline Control: Thixotropic flow and spacer beads support consistent adhesive placement.
  • Fast Handling Strength Development: The mixed adhesive reaches handling strength in about 20 minutes at 23 deg C.

Applications

Panel and frame bonding, thin-panel assembly, and joining compatible dissimilar substrates in transportation and industrial structures.

Product Family

3M DP8610NS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (Base / Accelerator)
Other Properties
Storage Temperature
16 - 27 °C
Thermal Properties
Glass Transition Temperature (Tg)
27 °C
Thermal Conductivity
0.235 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Mix ratio by volume10:1B:ATwo-part system
Mix ratio by weight10:1B:ATwo-part system
Base colorBlack-Before mixing
Accelerator colorGray-Before mixing
Base viscosity35000 to 100000cPAt 23 deg C; cone-and-plate, 4 sec^-1
Accelerator viscosity8000 to 18000cPAt 23 deg C; cone-and-plate, 4 sec^-1
Work life7minMixed adhesive
Open time8minBefore closing and fixing the bond
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorBlack-Cured
Modulus25MPaASTM D638 / ISO 527 at 23 deg C
Elongation at break140%ASTM D638 / ISO 527 after 7 days
Hardness38Shore DASTM D2240 at 23 deg C
Overlap shear on aluminum6.8MPaASTM D1002; MEK, abrade, MEK; 72 h at 23 deg C
Overlap shear on fiber-reinforced epoxy10.1MPaASTM D1002; MEK, abrade, MEK; 72 h at 23 deg C
Bell peel on aluminum11N/mmASTM D3167; light abrasion and solvent clean