Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Structural Acrylic Adhesive DP8005

Main features

  • Room Temperature Cure
  • Excellent Water and Humidity Resistance
  • Very Good Chemical Resistance

Product Description

3M™ Scotch-Weld™ Structural Plastic Adhesive DP8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropylene, polyethylene, and TPO’s without special surface preparation.

3M™ Scotch-Weld Adhesive DP8005 can replace screws, rivets, plastic welding, and two-step processes which include chemical etchants, priming or surface treatments in many applications.

Product Key Features

  • Ability to Bond Dissimilar Substrates 
  • Ability to Structurally Bond Polyolefins 
  • Room Temperature Cure 
  • Excellent Water and Humidity Resistance 
  • Very Good Chemical Resistance 
  • One Step Process - No Pre-Treatment of the Substrates Needed 
  • Solvent-free Adhesive System 
  • Convenient Hand-Held Applicator System 
  • Contains 0.008” glass beads for bondline thickness control
Product Family

3M DP8005

1. Select Package Type
2. Select Color
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Color.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methacrylate/Amine
Color
Black/White
Mix Ratio
10:1
Work life @25°C
0.05 hours
Physical Properties
Viscosity
15,000 - 55,000 mPa.s