3M™ Scotch-Weld™ Epoxy Adhesive DP760
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 2:1 mix ratio
- Non sagging paste
- High temperature resistance
Product Description
3M Scotch-Weld™ DP760 epoxy adhesive is a non-sag, two-part room temperature curing adhesive designed for use when high temperature resistance is required.
Product Key Features
- Epoxy adhesive
- 2:1 mix ratio
- Non sagging paste for an ease of use
- High temperature resistance
Applications
- Powder Coating & Baking Lines: Bonding metal components that must withstand high-temperature curing ovens.
- Engine Compartment Assembly: Securing brackets, sensors, and structural components near high-heat automotive or aerospace zones.
- Industrial Oven Fabrication: Sealing joints and mounting hardware on commercial heating equipment.
- Metal Component Manufacturing: Replacing mechanical fasteners or welding in specialized heavy machinery prone to intense operational heat.
Technical Specifications
General Properties
Chemistry Type
Modified Epoxy/Modified Amine
Color
White
Mix Ratio
100:50
Specific Gravity
0.84 - 1.24
Work life @25°C
1.5 hours
Physical Properties
Thixotropic index
Non-sagging Paste