3M DP640

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M DP640

Main features

  • 40-Minute Working Window
  • Thixotropic Non-Sag Placement
  • 2,160 lb/in^2 Aluminum Overlap Shear

Product Description

3M™ Scotch-Weld™ Urethane Adhesive DP640 Brown is a two-part, non-sag polyurethane adhesive that forms tough, flexible bonds across a range of substrates. It is particularly suited to wood and many properly abraded and cleaned plastics, with documented adhesion to painted metals, ceramics, and glass. The 1:1 mix ratio and thixotropic consistency support controlled application, while a 40-minute work life and 60-minute open time provide an extended assembly window. At 23 °C, the adhesive reaches handling strength in approximately 6–8 hours and develops at least 80% of ultimate strength after 7 days. For maximum bond durability in moist conditions, glass surfaces require priming.

Key features

  • Tough, flexible bonding: Produces flexible cured bonds with 100% elongation and 75 Shore A hardness.
  • Extended assembly window: Provides a 40-minute work life and up to 60 minutes of open time.
  • Non-sag 1:1 formulation: Thixotropic consistency supports controlled dispensing on vertical and overhead surfaces.

Applications / Suitable for

  • Bonding wood
  • Bonding properly abraded and cleaned plastics
  • Bonding painted metals
  • Bonding ceramics and glass
  • Applications requiring a non-sag adhesive

Technical Specifications

General Properties
Appearance
Brown
Density (g)
B: 1.08–1.12/A: 1.14–1.19 g/cm3
Mix Ratio
1:1
Solids
100 %
Work life @25°C
400 mins hours
Physical Properties
Open time
60 minutes
Viscosity (Part A)
15,000-55,000 mPa.s
Viscosity (Part B)
10,000-40,000 mPa.s
Mechanical Properties
Elongation
100 %
Peel Strength
112 N/cm
Thermal Properties
Temperature Resistance
(-51)- 121 ˚C
Electrical Properties
Volume Resistivity
2.6 x 10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the individual components and mixed adhesive. These values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
Mixed color Brown — Typical mixed adhesive
Mix ratio by volume 1:1 B:A As supplied in a dual-component cartridge
Base density 10.0–10.5 lb/gal Base component
Accelerator density 11.1–11.5 lb/gal Accelerator component
Base viscosity 10,000–40,000 cP 27 °C; Brookfield RVF, spindle #6, 10 rpm
Accelerator viscosity 15,000–55,000 cP 27 °C; Brookfield RVF, spindle #6, 10 rpm
Work life 40 min 10 g mixed adhesive at 23 °C
Open time 60 min Maximum time after application before the bond is closed and fixed
Technical properties

After-processing / final-state properties

Typical cured and bonded performance values under the stated test conditions. Results may vary with substrate, preparation, bondline, and curing conditions.

Property Value Unit Method / condition
Cured color Brown — Typical cured adhesive
Shore A hardness 75 Shore A ASTM D2240 at 23 °C
Elongation 100 % ASTM D882
Overlap shear strength — aluminum 2,160 lb/in² ASTM D1002 / ISO 4587; 23 °C; 7-day dwell; MEK/abrade/MEK preparation
Overlap shear strength — cold-rolled steel 1,960 lb/in² ASTM D1002 / ISO 4587; 23 °C; 7-day dwell; MEK/abrade/MEK preparation
Overlap shear strength — ABS 1,729 lb/in² ASTM D1002 / ISO 4587; 23 °C; 7-day dwell; IPA wipe/abrade/IPA wipe
Bell peel 64 lb/in width ASTM D3167; aluminum substrate at 23 °C
Volume resistivity 2.6 × 10¹⁴ Ω-cm ASTM D257 at 23 °C

Leading Brands Trust in Our Products and Services