3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus

Main features

  • 2-5 minute work life
  • Good shear and excellent peel strength
  • Flexible

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus is a flexible, fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is unique among fast setting mercaptan cure epoxies in that it combines high shear strength with good peel performance properties. Scotch-Weld epoxy adhesive DP100 Plus Clear is clear when cured. Available in bulk containers as 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus B/A Clear.

Product Key Features

  • 2-5 minute worklife
  • Good shear and excellent peel strength
  • Flexible
  • 1:1 mix ratio
  • Recognized as meeting UL 94 HB
Product Family

3M DP100PLUS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Epoxy
Color
Clear, colorless to light yellow/amber
Mix Ratio
1:1
Mechanical Properties
Elongation
70 %
Physical Properties
Young's modulus
10.413 MPa