3M AF126-3

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M AF126-3

Main features

  • Low Temperature Cure
  • Controlled Low Flow Processing
  • Green Supported Film Handling

Product Description

3M Scotch-Weld Structural Adhesive Film AF 126-3 is a green, toughened epoxy structural adhesive film for bonding prepared metal, composite, and honeycomb assemblies. Its matte nonwoven scrim-supported construction combines low tack for handling with low flow for bondline control during cure. The film can cure at temperatures as low as 82 deg C, supporting lower-temperature processing where the complete assembly permits it. Metal preparation, primer selection, applied pressure, and the full time-and-temperature cure schedule define the complete bonding process.

Key features

  • Low Temperature Cure: The film can cure at temperatures as low as 82 deg C.
  • Low Flow Bondline Control: Controlled flow helps retain adhesive placement during cure.
  • Green Supported Construction: The matte nonwoven scrim provides handling support during layup.

Applications

Structural bonding of prepared metals, composites, and honeycomb sandwich assemblies.

Product Family

3M AF126-3

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green
Physical Properties
Volatiles
Less than 1 %
Other Properties
Storage Temperature
-18 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Film constructionMatte nonwoven scrim supported-AF 126-3
ColorGreen-As supplied
Nominal areal weight294g/m20.060 lb/ft2
Nominal caliper0.25mm0.010 in
Volatile contentLess than 1%As supplied
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile shear at 24 deg C37.2MPaAverage with EC-2320 primer
Tensile shear at 82 deg C18.8MPa10 min exposure; average with EC-2320 primer
Tensile shear at -55 deg C42.5MPa10 min exposure; average with EC-2320 primer
T-peel at 24 deg C156N/25 mmAverage with EC-2320 primer