3M Scotch-Weld Structural Adhesive Film AF 126 is a thermosetting, nonvolatile modified epoxy film adhesive for structural bonding of metals and honeycomb constructions. Supported film options with protective liners are available in several nominal weights and calipers, allowing the construction to be matched to the required bondline. The film can cure at temperatures as low as 107 deg C, with optimum results from a 121 deg C cure for 1 hour. Negligible volatile byproducts support low-pressure bonding, while uncured tack assists placement during layup.

Key features

  • Low Temperature Cure Option: The film can cure at temperatures as low as 107 deg C.
  • Low Volatile Cure: Negligible volatile byproducts support low-pressure structural bonding.
  • Multiple Film Weight Options: Supported constructions provide selectable nominal weight and caliper.

Applications

Structural bonding of prepared metals and honeycomb sandwich assemblies.

Product Family

3M AF126

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Volatiles
Less than 1 %
Other Properties
Storage Temperature
-18 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are listed by AF 126 film weight to preserve configuration context.

PropertyValueUnitMethod / condition
Film constructionSupported film with protective liners-AF 126 family
Nominal areal weight options147.1; 294.2; 392.3g/m20.030; 0.060; 0.080 lb/ft2 variants
Nominal caliper options0.127; 0.254; 0.381mmCorresponding weight variants
Color by weightGreen; green; red-Corresponding weight variants
Volatile contentLess than 1%As supplied
Technical properties

After-processing / final-state properties

Cured bond averages retain film-weight and EC-2320 primer context.

PropertyValueUnitMethod / condition
Tensile shear at 24 deg C, 0.030 wt31.9MPaAverage with EC-2320 primer
Tensile shear at 24 deg C, 0.060 wt38.6MPaAverage with EC-2320 primer
Tensile shear at 24 deg C, 0.080 wt36.8MPaAverage with EC-2320 primer
T-peel at 24 deg C, 0.030 wt133N/25 mmAverage with EC-2320 primer
T-peel at 24 deg C, 0.060 wt191.4N/25 mmAverage with EC-2320 primer
T-peel at 24 deg C, 0.080 wt164.7N/25 mmAverage with EC-2320 primer