3M™ Scotch-Weld™ Structural Adhesive Film AF 163-2 OST Version

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Structural Adhesive Film AF 163-2 OST Version

Main features

  • High Structural Bond Strength
  • High Fracture Toughness and Peel Strength
  • Low-Pressure and Vacuum Curing

Product Description

3M™ Scotch-Weld™ Structural Adhesive Film AF 163-2 is a family of thermosetting, modified epoxy structural adhesives supplied in film form with multiple weights and carrier options. Designed for solid-panel and honeycomb sandwich construction, the adhesive combines high bond strength across temperatures from -67°F to 250°F with high fracture toughness, peel strength, and resistance to high-moisture environments before and after cure. It supports low-pressure and vacuum curing and is X-ray opaque for use with X-ray nondestructive inspection methods.

Key Features

  • Wide-temperature bond performance: Provides high bond strength from -67°F to 250°F.
  • High toughness and peel strength: Formulated for structural assemblies requiring resistance to fracture and peeling forces.
  • Moisture-resistant performance: Maintains resistance to high-moisture environments before and after curing.
  • Flexible processing: Supports low-pressure bonding, vacuum curing, and a 90-minute cure at 225°F.
  • X-ray opaque: Enables inspection using X-ray nondestructive inspection methods.

Applications / Suitable for

  • Solid-panel structural bonding
  • Honeycomb sandwich construction
  • Metal-to-metal structural bonding
  • Metal-to-honeycomb structural assemblies
  • Bonding aluminum, titanium, stainless steel, and epoxy fiber-reinforced plastic under documented preparation and cure conditions
Product Family

3M AF 163-2 OST

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
108 °C
Thermal Conductivity
0.166 W/m.K
Electrical Properties
Dielectric Strength
18 kV/mm
Volume Resistivity
4.4 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Available film constructions, nominal weights, colors, thicknesses, and documented storage conditions. Available configurations vary by carrier type and product designation.

Property Value Unit Method / condition
Adhesive type Thermosetting modified epoxy structural adhesive film — As supplied
Nominal film weight 0.015–0.100 lb/ft² Depends on AF 163-2 construction; nominal tolerance ±0.005 lb/ft²
Nominal thickness 2.5–16 mil Depends on film weight and carrier construction
Available colors Pink, yellow, red, blue, or green — Depends on product construction and film weight
Carrier options Fiberglass scrim, knit, lightweight nonwoven, nonwoven, one-side-tacky nonwoven, or unsupported — G, K, L, M, OST, and U designations
Recommended cold-storage temperature 0 or below °F Recommended for maximum storage life
Standard shelf life 12 months Stored at 0°F or below
Out-of-cold-storage allowance 20 days 80°F maximum without adversely affecting performance

 

Technical properties

After-processing / final-state properties

Representative cured-film properties. Values are typical and depend on the selected film construction, substrate preparation, primer, cure cycle, pressure, heating rate, and test conditions.

Property Value Unit Method / condition
Ultimate tensile strength 11,000 at -67°F; 7,000 at 75°F; 3,000 at 180°F psi ASTM D638; unsupported free film, cured 60 minutes at 250°F
Tensile modulus 2.3 × 105 at -67°F; 1.6 × 105 at 75°F; 6 × 104 at 180°F psi ASTM D638; unsupported free film, cured 60 minutes at 250°F
Glass-transition temperature, dry 226 (108) °F (°C) DuPont 1090 DMA; 5°C/min ramp; cured 90 minutes at 235°F
Glass-transition temperature, wet 180 (82) °F (°C) DuPont 1090 DMA; after 14 days in 70°C water; 5°C/min ramp; cured 90 minutes at 235°F
Thermal conductivity 0.096 BTU·ft/(ft²·hr·°F) ASTM C177 at 43°C; cured 90 minutes at 235°F
Coefficient of thermal expansion 90 × 10-6 in/in/°C TMA at 5°C/min, -30°C to 50°C; cured 90 minutes at 235°F
Volume resistivity 4.4 × 1014 Ω·cm ASTM D257; cured 90 minutes at 235°F
Dielectric strength 1,800 V/mil ASTM D149; 1 kHz at 75°F (23°C); cured 90 minutes at 235°F

 