3M AC-770-B-2-3

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-770-B-2-3

Main features

  • Low Density Fuselage Sealing
  • Controlled Thixotropic Placement
  • Extended Class B Work Life

Product Description

3M Aerospace Sealant AC-770 Class B-2-3 is a two-part, low-density, manganese-dioxide-cured polysulfide sealant for aircraft fuselage sealing. Its thixotropic Class B paste supports extrusion, injection, and spatula placement while resisting flow after application. The system uses a 100:10 base-to-accelerator mix ratio by weight. Class B schedules include B-1 and B-2 grades, with B-2 providing a 2 hour application life at 77 deg F and 50% relative humidity. After cure, the dark-brown sealant remains flexible across a broad aerospace service temperature range.

Key features

  • Low Density Fuselage Sealing: The cured sealant combines a 1.10 specific gravity with aircraft joint sealing.
  • Thixotropic Application Control: Class B consistency supports extrusion, injection, and spatula placement.
  • Extended B2 Work Life: The B-2 schedule provides a 2 hour application life under controlled conditions.

Applications

Aircraft fuselage joint sealing by extrusion, injection, or spatula application.

Product Family

3M AC-770-B-2-3

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (Base / Accelerator)
Specific Gravity
1.10
Thermal Properties
Service temperature
-54 to 121 °C
Other Properties
Storage Temperature
Below 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Base colorOff white-Before mixing
Accelerator colorBrown-Before mixing
Mix ratio by weight100:10base:acceleratorClass B system
Nonvolatile content98.5%Typical
Base viscosity9500 to 13000poiseBrookfield RVT, spindle 7, 2 rpm, 77 deg F
B-2 schedule2; 7 to 8; 9 to 11hApplication life; tack-free time; cure time at 77 deg F and 50% relative humidity
Shelf life9monthsStored below 80 deg F
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorDark brown-Cured 14 days at 77 deg F and 50% relative humidity
Specific gravity1.10-Cured
Hardness42 to 48Shore ACured
Tensile strength250psiStandard cure
Elongation310%Standard cure
Service temperature range-54 to 121deg CCured sealant