3M AC-730

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-730

Main features

  • Non Chromated Corrosion Inhibition
  • Flowable And Thixotropic Options
  • Selectable Application Life Grades

Product Description

3M Aerospace Sealant AC-730 is a two-part, non-chromated, corrosion-inhibiting polysulfide sealant family for aircraft faying surfaces and joints. Class B grades are thixotropic pastes for extrusion, injection, or spatula placement, while Class C grades are flowable materials for fay-surface application. Both classes use a 100:10 base-to-accelerator mix ratio by weight. Multiple grade schedules let users select an application-life window for the assembly process. After cure, the sealant provides low-temperature flexibility and service capability from -54 to 121 deg C.

Key features

  • Non Chromated Corrosion Inhibition: The polysulfide system supports protected aircraft sealing without chromate inhibitor.
  • Class B And C Options: Thixotropic and flowable forms address different joint and faying-surface processes.
  • Selectable Application Life: Multiple grade schedules support short or extended assembly windows.

Applications

Aircraft faying-surface and joint sealing using the class and grade matched to the application method.

Technical Specifications

General Properties
Component System
Two (Base / Accelerator)
Specific Gravity
1.5
Other Properties
Storage Temperature
Below 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Class B and Class C values are separated to preserve their different application forms.

PropertyValueUnitMethod / condition
Mix ratio by weight100:10base:acceleratorClass B and Class C systems
Class B formThixotropic paste-Extrusion, injection, or spatula application
Class B base viscosity9500 to 16000poiseBrookfield RVT, spindle 7, 2 rpm, 25 deg C
Class B nonvolatile content98%Typical
Class C formFlowable-Fay-surface application
Class C base viscosity2000 to 4000poiseBrookfield RVT, spindle 7, 2 rpm, 25 deg C
Class C nonvolatile content90%Typical
Technical properties

After-processing / final-state properties

Final-state values retain their Class B or Class C test context.

PropertyValueUnitMethod / condition
Class B specific gravity1.52-Cured 14 days at 25 deg C and 50% relative humidity
Class C specific gravity1.5-Cured 14 days at 25 deg C and 50% relative humidity
Class B hardness50Shore ACured
Low-temperature flexibilityNo checking or adhesion loss-At -54 deg C
Service temperature range-54 to 121deg CCured sealant
Short-duration temperature range-54 to 182deg CCured sealant