3M AC-380

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-380

Main features

  • Fuel Tank Sealing Performance
  • Thixotropic Application Control
  • Selectable Assembly Work Life

Product Description

3M Aerospace Sealant AC-380 Class B is a two-part, manganese-dioxide-cured polysulfide sealant for aircraft fuel tank and fuselage sealing. The thixotropic Class B paste can be extruded, injected, or applied by spatula, helping it stay in place during assembly. B-1/2 and B-2 grades provide different application-life and cure schedules while sharing a 100:10 base-to-accelerator mix ratio by weight. After cure, the dark-gray sealant combines low density, flexible Shore A hardness, and service capability across a broad aerospace temperature range.

Key features

  • Fuel Tank Sealing: The polysulfide chemistry supports compatible aircraft fuel tank and fuselage joints.
  • Thixotropic Class B Paste: The mixed sealant supports extrusion, injection, and spatula application.
  • Selectable Work Life Grades: B-1/2 and B-2 schedules support different assembly windows.

Applications

Aircraft fuel tank and fuselage sealing by extrusion, injection, or spatula application.

Product Family

3M AC-380

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two (Base / Accelerator)
Specific Gravity
1.1
Thermal Properties
Service temperature
-62 to 121 °C
Other Properties
Storage Temperature
Below 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Base colorOff white-Before mixing
Accelerator colorBlack-Before mixing
Mix ratio by weight100:10base:acceleratorClass B system
Nonvolatile content97%Typical
Base viscosity10000 to 14000poiseBrookfield RVT, spindle 7, 2 rpm, 77 deg F
B-1/2 schedule0.5; 5; 5hApplication life; tack-free time; cure time at 77 deg F and 50% relative humidity
B-2 schedule2; 8 to 10; 8 to 10hApplication life; tack-free time; cure time at 77 deg F and 50% relative humidity
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorDark gray-Cured 14 days at 77 deg F and 50% relative humidity
Specific gravity1.1-Cured
Hardness45 to 50Shore ACured
Low-temperature flexibilityNo checking or adhesion loss-At -62 deg C
Service temperature range-62 to 121deg CCured sealant
Short-duration temperature range-62 to 182deg CCured sealant