Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-130-2

Main features

  • Non Chromated Metal Preparation
  • Ambient Dry Process
  • Brush Spray Or Immersion Application

Product Description

3M Surface Pre-Treatment AC-130-2 is a two-part, water-based, non-chromated sol-gel surface treatment for preparing aluminum alloys, steel, and titanium before adhesive bonding. The mixed treatment can be applied by brush, spray, or immersion and dries at ambient conditions without a rinse or heat-cure step. A 30 minute induction period prepares the mixture for use, followed by a 10 hour pot life. Applying the compatible primer or adhesive within 24 hours of treatment helps maintain the intended bonding process window.

Key features

  • Non Chromated Sol Gel: The water-based treatment prepares compatible metals without a chromate conversion step.
  • Ambient Dry Processing: Brush, spray, or immersion application requires no rinse or heat cure.
  • Flexible Metal Preparation: The treatment supports aluminum alloys, steel, and titanium bonding processes.

Applications

Surface preparation of aluminum alloys, steel, and titanium before compatible adhesive bonding.

Product Family

3M AC-130-2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
As mixed, it is slightly cloudy un-tinted
Pot Life
10 hours
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the mixed treatment before and during application.

PropertyValueUnitMethod / condition
System configurationTwo part-Mix before use
Mixed appearanceSlightly opaque and untinted-After mixing
Induction time30minBefore application
Pot life10hAfter induction
Application temperature14 to 31deg CBrush, spray, or immersion
Maximum relative humidity85%During application and drying
Primer or adhesive window24hAfter treatment