Main features
- 5 mil Adhesive 300 Construction
- High Initial Adhesion and Holding
- Multi-Substrate Pressure-Sensitive Bonding
Product Description
3M™ Adhesive Transfer Tape 950 is a 5 mil (0.13 mm) adhesive transfer tape featuring 3M™ Adhesive 300, a pressure-sensitive, medium-firm, fibered acrylic adhesive supplied on a tan 60# glassine liner. It provides very high initial adhesion with good holding power across a range of materials, including metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
Key features
- High initial adhesion: 3M™ Adhesive 300 provides strong initial bonding with good holding power.
- Broad substrate compatibility: Bonds to metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
- Conformable 5 mil adhesive: The 0.13 mm adhesive thickness supports bonding to surfaces where texture may be visible.
- Environmental resistance: Provides resistance to humidity, water, UV exposure, temperature cycling, oil, mild acids, and mild alkalis when properly applied.
- UL-recognized construction: Recognized under UL 969 for Marking and Labeling Systems Materials Components.
Applications / Suitable for
- Bonding graphic nameplates and overlays
- Attaching metal nameplates and rating plates
- Laminating foam for gasket applications
- Joining similar and dissimilar industrial materials
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Adhesive Layer
300 Fibered Acrylic
Release Liner
Tan 60# Glassine
Total Thickness
130 μm
Additional Information
Technical properties
As-supplied / before-processing properties
Representative or typical product properties. Values should not be used for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive type | 3M™ Adhesive 300, fibered acrylic | — | Pressure-sensitive, medium-firm acrylic |
| Total tape thickness | 0.13 (5) | mm (mil) | ASTM D3652 |
| Liner | 60# glassine | — | Tan primary liner |
| Liner thickness | 0.08 (3.2) | mm (mil) | Published typical value |
| 90° peel adhesion — ABS | 3.7 (34); 4.4 (40) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| 90° peel adhesion — polypropylene | 6.6 (60); 6.8 (62) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| 90° peel adhesion — stainless steel | 8.1 (74); 9.4 (86) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| Short-term temperature resistance | 121 (250) | °C (°F) | Short term: minutes or hours |
| Long-term temperature resistance | 70 (158) | °C (°F) | Long term: days or weeks |
| Lower temperature service limit | -40 (-40) | °C (°F) | Properly applied tape |
| Coefficient of thermal expansion — first heat | 20 × 10-5 | m/m/°C | ASTM D696 |
| Coefficient of thermal expansion — second heat | 58 × 10-5 | m/m/°C | ASTM D696 |
| Dielectric constant | 3.21 | — | ASTM D150; 23°C (73°F); 1 kHz |
| Dissipation factor | 0.04 | — | 23°C (73°F); 1 kHz |
| Dielectric strength | 340 | V/mil | ASTM D149; 500 VAC RMS, 60 Hz/sec |
| Shelf life | 24 | months | From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight |