3M 92

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 92

Main features

  • Polyimide Film with Silicone Adhesive
  • 6,000 V Dielectric Breakdown
  • UL-Recognized Flame-Retardant Tape

Product Description

3M™ Polyimide Film Electrical Tape 92 with Silicone Adhesive is an amber electrical tape constructed with a polyimide film backing and a non-corrosive, thermosetting silicone pressure-sensitive adhesive. The 2.75 mil (0.070 mm) tape is designed for continuous operation at temperatures not exceeding 180°C (356°F) per its UL listing. It is commonly used for electrical insulation, component wrapping, lead anchoring, and solder masking during printed circuit board assembly.

Key features

  • High-temperature electrical tape: Designed for continuous operation at temperatures not exceeding 180°C (356°F) per its UL listing.
  • Polyimide film construction: Combines a nominal 1 mil (0.025 mm) polyimide backing with a thermosetting silicone pressure-sensitive adhesive.
  • Electrical insulation performance: Provides a minimum dielectric breakdown of 6,000 V and minimum insulation resistance of 1 × 1012 Ω.
  • Non-corrosive adhesive: Delivers an electrolytic corrosion factor of 1.0, where 1.0 indicates no corrosion observed under 3M Test Method ETM-54001.
  • Pressure-sensitive application: Requires no heat, moisture, or other preparation to achieve application.

Applications / Suitable for

  • Wrapping coils, capacitors, wire harnesses, and transformers
  • Anchoring electrical leads
  • Solder masking during printed circuit board assembly
Product Family

3M 92

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
thermosetting silicone
Color
amber
Film Thickness
0.025 mm
Total Thickness
190 μm
Mechanical Properties
Adhesion Strength
18 Oz/in
Elongation
40 %
Electrical Properties
Breakdown Voltage
6,000 V

Additional Information

Technical properties

As-supplied / before-processing properties

Published product properties measured at 73°F (23°C) unless otherwise stated.

Property Value Unit Method / condition
Color Amber — Visual
Backing Polyimide film — As supplied
Adhesive Thermosetting silicone — Pressure-sensitive adhesive
Backing thickness, nominal 1 (0.025) mil (mm) Published nominal value
Total thickness 2.75 ± 0.75 (0.070 ± 0.019) mil (mm) ASTM D1000; 73°F (23°C)
Adhesion to steel, minimum 18 (2.0) oz/in (N/cm) ASTM D1000; 73°F (23°C)
Breaking strength, minimum 20 (35) lb/in (N/cm) ASTM D1000; 73°F (23°C)
Elongation, minimum 40 % ASTM D1000; 73°F (23°C)
Dielectric breakdown, minimum 6,000 V ASTM D1000; 73°F (23°C)
Insulation resistance, minimum 1 × 1012 Ω ASTM D1000; 73°F (23°C)
Electrolytic corrosion factor 1.0 — 3M ETM-54001; 1.0 indicates no corrosion observed
Flame retardancy Pass — UL Recognized flame retardant per UL 510A
Continuous operating temperature, maximum 180 (356) °C (°F) Per UL listing
Shelf life 5 years From date of manufacture; store at 50–80°F (10–27°C) and less than 75% relative humidity