3M 90CA

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 90CA

Main features

  • Fast Tack Spray Bonding
  • Adjustable Lace Spray Pattern
  • Broad Assembly Material Compatibility

Product Description

3M Hi-Strength 90 CA Spray Adhesive is a high-strength, fast-tacking spray contact adhesive for assembly and maintenance bonding. Its synthetic elastomer base delivers a clear adhesive layer with a variable lace spray pattern, helping users apply coverage across broad surfaces. A 1 to 4 minute dry time and a 1 to 30 minute bonding range support practical positioning before parts are joined. The low-VOC formulation is suited to regulated aerosol applications, while the adhesive bonds laminates, wood, fabrics, and many plastics when the substrate and process conditions are compatible.

Key features

  • Fast Tack Development: A short dry time supports efficient assembly before parts are joined.
  • Adjustable Lace Spray: The variable spray pattern helps control coverage across different work areas.
  • Broad Material Compatibility: The adhesive supports bonding of laminates, wood, fabrics, and many plastics.

Applications

General assembly, maintenance bonding, laminate attachment, fabric bonding, woodworking, and compatible plastic bonding.

Product Family

3M 90CA

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Translucent
Density (g)
0.72 g/cm3
Solids
13 %
Physical Properties
Dry Time
1 minutes
VOC
<55
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BaseSynthetic elastomer-As supplied
ColorClear-As supplied
Solids by weight23.2%Typical
Density7.3lb/galTypical
Dry time1 to 4minBefore bonding
Bonding range1 to 30minAfter spray application
Coverage50ft2/canAt 2.5 g/ft2 coating weight

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers