Product Description

3M Scotchcast Electrical Resin 8N is a two-part, unfilled liquid epoxy resin system for electrical and electronic coating, filling, insulation, and encapsulation. The semi-flexible material is designed for room-temperature cure, with a 30-minute gel time at 60 deg C. After cure, the resin has 68 Shore D hardness, a Class B temperature rating of 130 deg C, and 75% elongation. Its low-viscosity liquid form supports filling and encapsulation around complex electrical and electronic assemblies.

Key features

  • Low-viscosity unfilled epoxy: The liquid, unfilled epoxy form supports coating, filling, patching, and encapsulation around electrical components.
  • Room-temperature cure capability: The resin has a low gel point for room-temperature cure, with a 30-minute gel time at 60 deg C.
  • Semi-flexible cured properties: The cured resin combines 68 Shore D hardness with reported 75% elongation for electrical insulation and encapsulation use.

Applications

Applications include coating, filling, patching, insulating, and encapsulating coils, transformers, motors, modules, and electrical or electronic components.

Product Family

3M 8N

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear Amber
Component System
Two
Specific Gravity
1.12
Other Properties
Storage Temperature
20 - 30 °C
Mechanical Properties
Elongation
75 %
Electrical Properties
Volume Resistivity
10¹³ Ohms⋅cm

Additional Information

Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Hardness68Shore DCured resin
Temperature rating130deg CClass B temperature rating
Elongation75%Cured resin
FlexibilitySemi-flexibleCured material classification