3M 8979

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8979

Main features

  • Six-Month Outdoor Clean Removal
  • One-Year UV Exposure Resistance
  • Hand-Tear Conformable Repairs

Product Description

3M Performance Plus Duct Tape 8979 is an outdoor-capable polyethylene-film and cloth-scrim duct tape with rubber adhesive for temporary indoor and outdoor maintenance, sealing, and repair. The 0.29 mm tape tears by hand, conforms to irregular surfaces, and develops immediate initial stick on many surfaces. It removes with little or no adhesive residue from most opaque surfaces for up to six months after application and resists delamination and deterioration under outdoor UV exposure for up to one year. Typical performance includes 6.2 N/cm peel adhesion, 64 N/cm tensile strength, and 17% elongation.

Key features

  • Six-month outdoor clean removal: The tape removes with little or no adhesive residue from most opaque surfaces for up to six months after application.
  • One-year outdoor exposure resistance: The construction resists UV-related delamination and deterioration outdoors for up to one year.
  • Hand-tear conformable backing: Polyethylene film over cloth scrim tears by hand and follows irregular surfaces for temporary repairs and sealing.

Applications

Applications include temporary weather sealing, pipe and conduit capping, patching, bundling, reinforcing, insulation splicing, marking, labeling, and temporary repair.

Product Family

3M 8979

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Slate Blue, Black, Olive
Total Thickness
290 μm
Mechanical Properties
Elongation
17 %
Tensile Strength (Thin Film)
64 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyethylene film over cloth scrimAs supplied
Adhesive typeRubberPressure-sensitive
Total tape thickness0.29mmASTM D3652; typical
ColorsSlate Blue, Black, OliveAvailable colors
Shelf life18monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion6.2N/cmASTM D3330; 23 deg C; typical
Elongation at break17%ASTM D3759; typical
Tensile strength64N/cmASTM D3759; typical
Clean removal windowUp to 6monthsMost opaque surfaces; indoor or outdoor exposure
Outdoor UV exposure resistanceUp to 1yearResistance to delamination and deterioration