3M 8417

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 8417

Main features

  • Transparent Self-Wound Polyester Film
  • Edge-Tear-Resistant Film Backing
  • -40 to 93 deg C Exposure Range

Product Description

3M™ PET Durable Label Material 8417 is a transparent, self-wound polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. Commonly used as an overlaminate with 3M™ PET Durable Label Material 8418, it provides instant adhesion, transparency, and a tough film backing that resists edge tearing during processing and dispensing. The construction also offers documented chemical resistance and stability across elevated and low-temperature exposure conditions, supporting durable identification applications where environmental resistance is required. :contentReference[oaicite:0]{index=0}

Key features

  • Transparent overlaminate construction: Clear polyester film preserves label visibility when used as an overlaminate.
  • Durable film backing: Tough polyester resists edge tearing during processing and dispensing.
  • Environmental resistance: Documented exposure testing shows no appearance change after selected chemical, humidity, and temperature conditions.

Applications / Suitable for

  • Overlaminating 3M™ PET Durable Label Material 8418
  • Fluid-line identification
  • General identification applications requiring chemical and temperature resistance
Product Family

3M 8417

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
3M™ Adhesive 100 High-temperature Acrylic
Adhesive Thickness
30 µm
Film Thickness
0.025 mm
Total Thickness
56 μm
Mechanical Properties
Elongation
100 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, dimensional, dispensing, and storage properties of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Construction Self-wound transparent polyester film — Linerless construction
Adhesive type 3M™ Adhesive 100 High-temperature Acrylic — Typical construction
Total tape thickness 0.056 (2.2) mm (mil) ASTM D3652; nominal caliper
Adhesive thickness 0.03 (1.2) mm (mil) Nominal caliper
Facestock thickness 0.025 (1) mm (mil) Polyester facestock; nominal caliper
Typical unwind 3 (3) oz/in (N/100 mm) Shocky unwind
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging away from direct sunlight

 

Technical properties

After-processing / final-state properties

Typical adhesion, mechanical, chemical, and temperature-exposure characteristics of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
180° peel adhesion — ABS 3.8 (35) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — glass 4.9 (45) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — polypropylene 1.2 (11) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
180° peel adhesion — stainless steel 4.1 (38) N/cm (oz/in) ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min)
Tensile strength 43.5 (400) N/cm (oz/in) Typical
Elongation at break 100 % Typical
Chemical exposure appearance No change — 4 h immersion at room conditions; 2 × 2 in samples on stainless steel; tested with isopropyl alcohol, 10W30 oil, pH 4 acid, pH 10 base, and water; zero edge penetration
Temperature-exposure appearance No change — 24 h exposure; 2 × 2 in samples on stainless steel; tested from -40°C (-40°F) to 93°C (200°F); selected conditions also evaluated at 90% RH