3M 78

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 78

Main features

  • EPS and Insulation Material Bonding
  • Aerosol or Cylinder Spray Delivery
  • Foundation and Foam-Core Applications

Product Description

3M Polystyrene Foam Insulation Spray Adhesive 78 is a single-component industrial spray adhesive for bonding expanded polystyrene and insulation materials. It is supplied in aerosol and cylinder delivery configurations for foam and insulation assembly work. The product is used in foundation insulation, polystyrene-block assembly, foam-to-wood bonding, roofing, landscaping, and foam-core construction. Aerosol and cylinder formats provide spray delivery for foundation insulation and foam-fabrication work. As a single-component product, it does not require a second adhesive component to be mixed before spray application.

Key features

  • EPS and insulation bonding: The spray adhesive is developed for expanded polystyrene and insulation materials in construction and foam assembly.
  • Aerosol and cylinder delivery: Aerosol and cylinder formats provide spray delivery for insulation and foam fabrication workflows.
  • Construction and foam assembly: The product is used for foundation insulation, foam-to-wood bonding, roofing, landscaping, and foam-core assembly.

Applications

Applications include foundation insulation, polystyrene-block assembly, foam-to-wood bonding, roofing, landscaping, and foam-core assembly.

Product Family

3M 78

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Translucent
Solids
19.1 %
Physical Properties
Dry Time
1 - 2 minutes
VOC
62.1 %
Other Properties
Storage Temperature
16 - 27 °C