3M 76

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M 76

Main features

  • High-Tack Industrial Formulation Excels in One-Surface Bonding
  • Polyethylene and Polypropylene Bonding
  • Controlled Variable Lace Spray Pattern

Product Description

3M™ Hi-Tack 76 Spray Adhesive is an industrial aerosol spray adhesive formulated with high tack for single-surface bonding applications. This translucent, synthetic elastomer-based adhesive effectively bonds hard-to-hold materials such as polyethylene and polypropylene. It provides a variable lace spray pattern and is an excellent choice for adhering fabric headliners, rubber, felt, plastics, and foil to themselves or to wood and metal surfaces.

Key features

  • High-tack performance: Formulated specifically for efficient one-surface bonding applications with a rapid 1-2 minute dry time.
  • Bonds difficult substrates: Effectively adheres to hard-to-hold plastics, including polyethylene and polypropylene.
  • Variable lace spray: Aerosol delivery provides a controlled variable lace pattern for precise application and a coverage of up to 2.6 m² (28 ft²) per can.

Applications / Suitable for

  • One-surface bonding applications
  • Bonding polyethylene and polypropylene plastics
  • Attaching fabric headliners
  • Bonding rubber, felt, cardboard, cork, and foil to wood or metal
Product Family

3M 76

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent
Chemistry Type
Synthetic Elastomer
Density (g)
0.78 g/cm3
Solids
13.5 %
Physical Properties
Dry Time
1-2 minutes
VOC
<55
Thermal Properties
Shear Adhesion Failure Test - SAFT
110 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Synthetic Elastomer - -
Color Translucent - -
Spray Pattern Variable Lace - -
Solids Content by Weight 13.5 % -
Density 0.78 kg/L (6.5 lb/gal)
Coverage 2.6 m² (28 ft²) at 27 g/m² dry
Dry Time 1-2 minutes Dependent on ambient conditions and coverage
Bonding Range 1-10 minutes 1 surface
Bonding Range 1-60 minutes 2 surfaces
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Shear Adhesion Failure Test (SAFT) 110 °C 230°F (birch plywood, 25 mm overlap, 100 g)