3M 70

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 70

Main features

  • Instant Self-Fusing Cable Overwrap
  • Class H High-Temperature Insulation
  • Arc-Resistant High-Voltage Protection

Product Description

Scotch Self-Fusing Silicone Rubber Electrical Tape 70 is a high-temperature, self-fusing inorganic silicone rubber tape for electrical insulation and protective overwrapping. It fuses to itself without a pressure-sensitive adhesive and uses an easy-tear, easy-strip liner for hand application. The tape provides high dielectric strength with arc and track resistance and is a Class H material for continuous operation at 180 deg C. Applied in half-lapped layers with moderate tension, it forms a fused protective wrap for high-voltage cable and other high-temperature electrical insulation work.

Key features

  • Instant self-fusion: The silicone rubber fuses to itself without a pressure-sensitive adhesive and does not need to be held down after wrapping.
  • Class H temperature capability: The 180 deg C continuous Class H rating applies to high-temperature primary insulation applications.
  • Arc and track resistance: High dielectric strength with arc and track resistance suits protective overwraps on high-voltage terminations.

Applications

Applications include high-voltage cable termination overwraps, Class H primary insulation, spacer-cable splice overwraps, and outdoor electrical protection.

Product Family

3M 70

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Munsell 5BG7.0/0.4 Sky Blue Grey
Total Thickness
300 μm
Mechanical Properties
Elongation
450 %
Electrical Properties
Arc Resistance
60 s
Dielectric Strength
34 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorSky Blue GrayMunsell 5BG7.0/0.4
Thickness0.012inTypical; ASTM D1000-10
Tensile strength12lb/inTypical; ASTM D1000-10
Elongation at break450%Typical; ASTM D1000-10
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Dielectric strength875V/milTypical; ASTM D1000-10
Arc resistance>= 1minTypical; ASTM D495-71
Continuous operating temperature180deg CClass H material