3M 5952

Main features

  • 45-Mil Conformable Foam Bonding
  • Painted-Surface Permanent Attachment
  • Panel and Display Assembly Bonding

Product Description

3M VHB Tape 5952 is a black, double-sided modified acrylic foam bonding tape with a 45 mil nominal thickness for permanent attachment to painted and powder-coated surfaces. Its conformable acrylic foam core is paired with modified acrylic adhesive on both sides and a release liner for pre-application handling. The continuous foam-tape construction is used to join panels, trim, stiffeners, displays, and frames where a conformable permanent bond is required. The product is supplied in multiple widths, lengths, and converted formats for configuration-specific industrial assembly needs.

Key features

  • 45 mil foam construction: The black double-sided tape combines 45 mil nominal thickness with a conformable acrylic foam core.
  • Painted-surface attachment: Modified acrylic adhesive supports permanent bonding to documented painted and powder-coated surfaces.
  • Panel and display assembly: The tape is used to join panels, trim, stiffeners, displays, and frames in documented assemblies.

Applications

Applications include permanent bonding of panels, trim, stiffeners, displays, and frames to documented painted and powder-coated surfaces.

Product Family

3M 5952

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Modified Acrylic
Color
Black
Density
590 kg/m3
Release Liner
PE Film
Total Thickness
1100 μm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBlackTape body
Adhesive typeModified acrylicBoth sides
CoreConformable acrylic foamDouble-sided construction
Nominal tape thickness45milProduct type record
Release linerPresentLinered construction