3M 5925

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 5925

Main features

  • Immediate Painted-Surface Bonding
  • Conformable 0.6 mm Foam Attachment
  • 93 deg C Long-Term Use

Product Description

3M VHB Tape 5925 is a black, double-sided modified acrylic foam tape for permanent attachment on painted and powder-coated surfaces. Its conformable foam core and modified acrylic adhesive provide a 0.6 mm applied thickness and immediate handling strength without a curing step. The tape combines high shear strength, conformability, and surface adhesion and is rated for long-term use up to 93 deg C. It is used for trim, nameplates, electronic displays, panel-to-frame and stiffener-to-panel bonding, with documented adhesion to materials including stainless steel and other compatible surfaces.

Key features

  • Immediate painted-surface handling: The modified acrylic construction bonds many painted and powder-coated surfaces with immediate handling strength and no cure wait.
  • Conformable 0.6 mm foam: The foam core provides a 0.6 mm applied bonding layer that conforms across the joined surfaces.
  • Long-term 93 deg C use: The tape is rated for long-term use at temperatures up to 93 deg C.

Applications

Applications include bonding trim, nameplates, electronic displays, panels, frames, and stiffeners, including permanent attachment to painted and powder-coated surfaces.

Product Family

3M 5925

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Modified Acrylic
Color
Black
Density
590 kg/m3
Release Liner
PE Film
Total Thickness
600 μm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBlackTape body
Adhesive typeModified acrylicBoth sides
CoreConformable acrylic foamDouble-sided construction
Total tape thickness0.6mm25 mil; applied tape
Liner materialPolyethylene filmRelease liner