3M 4950

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4950

Main features

  • Immediate No-Cure Assembly Handling
  • Firm 1.1 mm Foam Bonding
  • High-Surface-Energy Permanent Attachment

Product Description

3M VHB Tape 4950 is a white, double-sided acrylic foam tape for permanent bonding of metals, glass, and other high-surface-energy materials. A firm acrylic foam core with general-purpose acrylic adhesive provides a 1.1 mm tape thickness and immediate handling strength without a fixturing or cure wait. The tape is rated for long-term use up to 93 deg C and short-term exposure up to 149 deg C for up to four hours. Its permanent bonding format is used for stiffener-to-panel and panel-to-frame attachment, decorative trim, nameplates, and logos.

Key features

  • Immediate no-cure handling: Pressure-sensitive all-acrylic bonding develops immediate handling strength without a fixturing or cure wait.
  • Firm 1.1 mm foam core: The firm acrylic foam construction provides a 1.1 mm double-sided bonding layer for permanent attachment.
  • High-surface-energy bonding: General-purpose acrylic adhesive bonds metals, glass, and other documented high-surface-energy substrates.

Applications

Applications include stiffener-to-panel bonding, panel-to-frame attachment, decorative trim, nameplates, and logos.

Product Family

3M 4950

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Density
800 kg/m3
Total Thickness
1100 μm
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhiteTape body
Adhesive typeGeneral-purpose acrylicBoth sides
CoreFirm acrylic foamDouble-sided construction
Total tape thickness1.1mm45 mil; product thickness
Liner materialDensified kraft paperRelease liner