3M 4926

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 4926

Main features

  • Conformable 0.4 mm Acrylic Foam
  • Multi-Purpose Acrylic Adhesive
  • 620 Kpa Overlap Shear Strength

Product Description

3M™ VHB™ Tape 4926 is a gray, 0.4 mm (0.015 in) double-sided acrylic foam tape for permanent bonding. Its multi-purpose acrylic adhesive bonds to a broad range of high- and medium-surface-energy substrates, including metals, glass, paints, plastics, and plasticized vinyl. The conformable foam core promotes contact between slightly mismatched surfaces, while the pressure-sensitive adhesive develops immediate handling strength upon application. The tape provides a smooth, virtually invisible fastening method and may replace selected rivets, welds, screws, or liquid adhesives when the complete joint design and application conditions are properly evaluated. :contentReference[oaicite:0]{index=0}

Key features

  • Conformable acrylic foam construction: The 0.4 mm foam tape promotes adhesive contact when bonded surfaces are slightly mismatched.
  • Multi-purpose substrate bonding: Bonds to high- and medium-surface-energy substrates, including metals, glass, paints, plastics, and plasticized vinyl.
  • Immediate handling strength: Pressure-sensitive adhesive bonds on contact, with bond strength continuing to build after application.

Applications / Suitable for

  • Permanent bonding of metals and glass
  • Bonding painted and selected plastic surfaces
  • Bonding selected plasticized-vinyl formulations following application-specific evaluation
  • Smooth, virtually invisible fastening
  • Evaluation as an alternative to selected mechanical fasteners or liquid adhesives
Product Family

3M 4926

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Color
Gray
Density
720 kg/m3
Release Liner
DK Paper
Single or Double-Sided Adhesive
Double
Total Thickness
400 μm
Mechanical Properties
Adhesion Strength
25 Oz/in
Thermal Properties
Operating Temperature
15-149 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction and physical properties of 3M™ VHB™ Tape 4926 as supplied. Values are representative and are not intended for specification purposes. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Color Gray — Typical
Adhesive type Multi-purpose acrylic — Adhesive on both sides
Foam type Conformable acrylic foam — Typical construction
Density 720 (45) kg/m³ (lb/ft³) ASTM D3574; foam with adhesive
Total tape thickness 0.4 (0.015; 15) mm (in; mil) ASTM D3652; thickness tolerance ±15%
Liner White printed DK paper — Liner thickness: 0.08 mm (0.003 in; 3 mil)
Minimum application temperature 15 (60) °C (°F) Tape and substrates should be conditioned at or above the minimum application temperature
Technical properties

After-processing / final-state properties

Typical performance characteristics of 3M™ VHB™ Tape 4926. Adhesion and strength values were measured at 23°C (73°F) after 72 hours of dwell unless otherwise stated. Values are representative and are not intended for specification purposes. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
90° peel adhesion 25 (14) N/cm (lb/in) ASTM D3330; stainless steel; 5 mil aluminum-foil backing; 304 mm/min (12 in/min)
Normal tensile strength 660 (95) kPa (lb/in²) ASTM D897; aluminum; 6.45 cm² (1 in²) bond area; jaw speed 51 mm/min (2 in/min)
Overlap shear strength 620 (90) kPa (lb/in²) ASTM D1002 / ISO 4587; stainless steel; 6.45 cm² (1 in²) bond area; jaw speed 12.7 mm/min (0.5 in/min)
Static shear holding 1,000 g ASTM D3654; stainless steel; 23°C (73°F); 3.23 cm² (0.5 in²); holds load for 10,000 min
Static shear holding at elevated temperature 500 g ASTM D3654; stainless steel; tested at 66°C (150°F) and 93°C (200°F); 3.23 cm² (0.5 in²); holds load for 10,000 min
Short-term temperature resistance 149 (300) °C (°F) No change in room-temperature dynamic shear properties after 4 h conditioning with a 100 g static load; process-type exposure
Long-term temperature resistance 93 (200) °C (°F) Maximum temperature supporting at least 78 g/cm² (500 g/in²) in static shear for 10,000 min; continuous exposure for days or weeks

Leading Brands Trust in Our Products and Services