3M 401M

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 401M

Main features

  • Fast High-Initial Substrate Grab
  • Fast Hand-Tearable Process Handling
  • Defined -40 to 65 deg C Service

Product Description

3M Double Coated Paper Tape 401M is a natural, 9 mil (0.228 mm) double-coated paper tape with rubber-resin pressure-sensitive adhesive for temporary attachment, splicing, and project stabilization. Its soft adhesive develops high initial adhesion and good holding power on a wide range of materials, while the paper carrier adds handling strength and permits hand tearing. The liner improves dimensional stability for die-cutting and automated dispensing and helps control edge roll during processing. After proper room-temperature application, the tape performs from -40 to 150 deg F (-40 to 65 deg C) in long-term service. Applications include splicing paper, foil, film, and fabric, mounting printing plates, attaching golf grips, and temporary part holding.

Key features

  • High-Initial Rubber Adhesion: The soft rubber-resin adhesive provides quick grab and good holding power.
  • Hand-Tearable Paper Carrier: The paper construction adds handling strength and tears by hand during application.
  • Stable Die-Cutting Liner: The densified kraft liner adds dimensional stability and helps reduce edge roll.

Applications

Suitable for splicing and core starting of paper, foil, film, and fabric; printing-plate mounting; golf-grip attachment; and temporary part holding.

Product Family

3M 401M

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White/Green
Other Properties
Storage Temperature
21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AdhesiveNatural rubber-Pressure-sensitive
CarrierPaper-Double coated
ColorNatural-As supplied
Total thickness without liner9 (0.228)mil (mm)As supplied
Adhesive thickness per side3 (0.08)mil (mm)As supplied
LinerDensified kraft paper-White and green
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Long-term temperature range-40 to 150 (-40 to 65)deg F (deg C)Properly applied tape
Initial adhesionHigh-Room-temperature application
Holding powerGood-Applied tape
Initial bondQuick grab-Pressure-sensitive application

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers