3M 3950

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3950

Main features

  • Film Edge-Lift Protection
  • Water-Tight Interface Sealing
  • Defined 50-100 deg F Application

Product Description

3M Edge Sealer 3950 is a colorless liquid acrylic sealant for exposed edges of compatible graphic films and screen-printing inks. Applied along the film boundary, it forms a water- and contaminant-tight seal that helps prevent edge lifting during environmental exposure or cleaning. The sealer is intended for application between 50 and 100 deg F and should not be applied directly to painted surfaces. Its liquid form reaches the narrow film-to-substrate interface for controlled edge coverage. This product suits graphics and screen-printing installations that face rigorous use, prolonged exposure, or repeated cleaning and require added protection at vulnerable film edges.

Key features

  • Film Edge-Lift Protection: The applied sealer helps keep compatible film edges from lifting during exposure or cleaning.
  • Water-Tight Interface Seal: The seal limits water and contaminant entry at the film-to-substrate boundary.
  • Defined Application Window: Apply between 50 and 100 deg F and not directly onto painted surfaces.

Applications

Suitable for sealing exposed edges of compatible graphic films and screen-printing inks.

Product Family

3M 3950

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear liquid
Solids
46 +/- 2.5 %
Physical Properties
Viscosity
300 mPa.s
Thermal Properties
Service temperature
-51 to + 65 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Physical stateLiquid-As supplied
ColorColorless-As supplied
OdorSlight solvent-As supplied
Density0.97g/mlAs supplied
Flash point25deg CTagliabue closed cup
Application temperature50 to 100deg FDo not apply directly to painted surfaces
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Edge-lift protectionHelps prevent lifting-Environmental exposure or cleaning
Water sealTight-Compatible graphic film and substrate
Contaminant sealTight-Compatible graphic film and substrate

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers