3M 3901

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 3901

Main features

  • Low-Viscosity Surface Wetting
  • Quick-Drying One-Component Application
  • Improved Metal Corrosion Protection

Product Description

3M Scotch-Weld Metal Primer 3901 is a red, low-viscosity, one-component liquid primer for preparing metal and glass before bonding with compatible 3M Scotch-Weld film and liquid structural adhesives. It wets treated surfaces thoroughly and dries quickly, simplifying application before adhesive placement. The primer helps maintain cleaned surfaces in a relatively oxidation-free condition until bonding is completed. In the bonded interface, it improves adhesion and resistance to environmental exposure while adding corrosion protection on metal. The 3 to 8 cP viscosity supports thin, even coverage for glass and metal assemblies that require controlled primer application and dependable structural-adhesive preparation.

Key features

  • Low-Viscosity Surface Wetting: The 3 to 8 cP liquid spreads readily for complete wetting before adhesive placement.
  • Quick-Drying One-Component Application: The ready-to-use primer simplifies surface preparation without component mixing.
  • Metal Corrosion Protection: The dried primer improves resistance to corrosion and environmental exposure on metal.

Applications

Suitable for priming metal and glass before compatible 3M Scotch-Weld film and liquid structural adhesives.

Product Family

3M 3901

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Red
Physical Properties
Viscosity
5 ± 2 mPa.s
Other Properties
Storage Temperature
16 -27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Physical stateLiquid-As supplied
ColorRed-As supplied
Viscosity3 to 8cPAs supplied
Density0.80g/mlAs supplied
Flash point52deg FClosed cup
Boiling point148deg FAs supplied
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Adhesion functionImproves metal and glass adhesion-Compatible 3M film and liquid structural adhesives
Corrosion protectionImproved-Metal surfaces
Environmental-exposure resistanceImproved-Primed metal interface
Cleaned-surface protectionMaintains relatively oxidation-free condition-Until bonding is completed