3M 3764-Q

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3764-Q

Main features

  • Quadrack-Format Controlled Dispensing
  • Rapid Seconds-Scale Bond Development
  • Flexible Impact-Resistant Bond

Product Description

3M Hot Melt Adhesive 3764 Q is a clear, 100% solids thermoplastic adhesive supplied in Q/Quadrack-stick form for use with compatible hot-melt applicators. Its molten phase wets many plastics, including polyolefins, and the adhesive hardens within seconds as it cools. A 50-second open time provides a controlled interval for positioning parts before bond development. The formulation is flexible at low temperatures, impact resistant, and characterized by good shear and peel strength. It is used for assembly, attaching, securing, repair, potting, panel bonding, wire tacking, bundling, sealing, encapsulating, and packaging across compatible plastic, metal, paper, cardboard, foam, ceramic, glass, PVC, and wood substrates.

Key features

  • Quadrack Applicator Compatibility: The Q-format stick is made for compatible 3M Quadrack hot-melt applicators.
  • Rapid Cooling Set: Bond strength develops within seconds as the molten adhesive cools and hardens.
  • Broad Substrate Bonding: The adhesive bonds many plastics, including polyolefins, plus compatible industrial materials.

Applications

Suitable for assembly, attaching, securing, repair, potting, panel bonding, wire tacking, bundling, sealing, encapsulating, and packaging.

Product Family

3M 3764-Q

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear
Density (g)
0.95 g/cm3
Thermal Properties
Flash Point
268 °C
Physical Properties
Viscosity
6,000 mPa.s
Chemical Properties
Melting Point
88 °C
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Product formQuadrack stick-As supplied
ColorTransparent-As supplied
Solids100% by weightApproximate
Open time50sHot-melt application
Application methodHandheld applicator-Compatible 3M Quadrack applicator
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Shear strength390psiMethod and condition not stated
Heat resistance temperature140 (60)deg F (deg C)Product classification
Bond-strength characterGood shear and peel strength-Cooled bond
Impact responseImpact resistant-Cooled bond
Low-temperature responseFlexible-Cooled bond