3M 3549

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3549

Main features

  • Non-Sag Vertical Bonding
  • Balanced 1:1 Mixing
  • Tough Low-Temperature Flexibility

Product Description

3M Scotch-Weld Urethane Adhesive 3549 is a brown, two-component polyurethane adhesive that becomes a non-sag paste after 1:1 mixing for vertical and other bead-controlled bonding. The tough, flexible cured adhesive joins dissimilar materials, including composites, SMC, FRP, plastics, ceramic, wood, rubber, concrete, and metal. Its positioning window allows panel adjustment before set, while low-temperature flexibility suits joints that require a resilient response. The adhesive reaches set or handling strength in 8 hours and full cure in 7 days under the listed timing. It is suited to panel-to-frame, door-frame, and wood-panel bonding where controlled placement and flexible adhesion are important.

Key features

  • Non-sag mixed paste: The combined urethane holds its bead in vertical and other slump-sensitive applications.
  • Balanced 1:1 mixing: Parts A and B combine at a one-to-one ratio before application.
  • Tough flexible cure: The cured adhesive provides flexible bonding and low-temperature flexibility.

Applications

Suitable for bonding composites, SMC, FRP, plastics, ceramic, wood, rubber, concrete, masonry, and metal, including panel-to-frame and door-frame assemblies.

Product Family

3M 3549

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Other Properties
Storage Temperature
15 - 27 °C
Mechanical Properties
Elongation
100 %
Electrical Properties
Volume Resistivity
2.6 x 10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ComponentsPart A and Part B-Before mixing
Mix ratio1:1-Before application
ColorBrown-Mixed adhesive
Mixed formNon-sag paste-After mixing
Specific gravity1.31-Condition not stated
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Set / handling strength8hCondition not stated
Full cure7daysCondition not stated
Shear strength2,000psiMethod and condition not stated
Cured responseLow-temperature flexibility-Cured adhesive