3M 3302

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3302

Main features

  • Low-Resistance Conductive Bonding
  • Conformable EMI/RFI Shielding
  • UL 510 Recognized Construction

Product Description

3M Conductive Aluminum Foil Tape 3302 is a silver, dead-soft aluminum foil tape with a conductive pressure-sensitive acrylic adhesive for low-level EMI/RFI shielding and printed-circuit manufacturing or repair. The 2 mil (0.05 mm) high-strength foil is malleable enough to follow irregular and textured surfaces, while the adhesive wets out to low-surface-energy materials and supports a low-resistance conductive bond. The 3.5 mil (0.09 mm) total construction is hand tearable for installation and carries UL 510 recognition. Applied performance includes typical peel and tensile data with long-term temperature resistance from -40 to 250 deg F (-40 to 121 deg C).

Key features

  • Conductive acrylic interface: The adhesive supports low-resistance bonding and electrical continuity across the applied tape.
  • Malleable dead-soft foil: The aluminum backing follows irregular, uneven, and difficult textured surfaces.
  • Wide long-term temperature range: Applied tape is rated from -40 to 250 deg F (-40 to 121 deg C) for days or weeks.

Applications

Suitable for low-level EMI/RFI shielding, printed-circuit manufacturing and repair, grounding, and electrical-continuity applications.

Product Family

3M 3302

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Silver
Mechanical Properties
Elongation
3 %
Tensile Strength (Thin Film)
33.3 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorSilver-Typical
AdhesiveConductive acrylic-Pressure-sensitive
BackingDead-soft aluminum foil-As supplied
Backing thickness0.05 (2)mm (mil)Typical; ASTM D3652
Total tape thickness0.09 (3.5)mm (mil)Typical; ASTM D3652
Liner thickness0.11 (4.4)mm (mil)Typical
Shelf life12monthsFrom manufacture; 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

Performance values are typical; methods and conditions are shown in each row.

PropertyValueUnitMethod / condition
180 deg peel adhesion2.4 (21)N/cm (oz/in)Typical; ASTM D3330 at 23 deg C and 304 mm/min
Elongation at break3%Typical; ASTM D3759
Tensile strength33.3 (19)N/cm (lb/in)Typical; ASTM D3759
Long-term temperature range-40 to 121 (-40 to 250)deg C (deg F)Days or weeks
RecognitionUL 510-File E230409

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers