3M 305

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 305

Main features

  • Instant Acrylic Carton Closure
  • Split-Resistant BOPP Handling
  • Cold-Temperature Packaging Use

Product Description

Tartan Box Sealing Tape 305 is a 1.8 mil (0.046 mm) biaxially oriented polypropylene tape with a pressure-sensitive acrylic adhesive for general-purpose carton closure. The conformable backing wraps edges and rough recycled corrugate while resisting abrasion, moisture, scuffing, edge tear, and splitting during application. Instant adhesion requires no moisture, heat, or solvent activation, supporting smooth hand dispensing, manual dispensers, and case-sealing equipment. The clear or tan tape is intended for lightweight boxes exposed to minimal distribution hazards and performs in cold-temperature packaging work. It also resists yellowing, weathering, and UV exposure in lightweight carton-sealing service.

Key features

  • Conformable BOPP backing: The polypropylene film follows carton edges and rough recycled corrugate for a tight closure.
  • Instant acrylic adhesion: The pressure-sensitive adhesive requires no moisture, heat, or solvent activation.
  • Split-resistant handling: The backing provides edge-tear and split resistance during carton-sealing application.

Applications

Suitable for lightweight carton sealing, food and beverage packaging, recycled liner paper and fiberboard, cold-temperature use, bag closure, and cartons exposed to UV light and aging.

Product Family

3M 305

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Pressure Sensitive Acrylic
Color
Clear and Tan
Film Thickness
0.025 mm
Total Thickness
46 μm
Mechanical Properties
Adhesion Strength
16.2 Oz/in
Tensile Strength (Thin Film)
701 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorClear and tan-Typical
AdhesivePressure-sensitive acrylic-As supplied
BackingBiaxially oriented polypropylene film-As supplied
Backing thickness0.025 (1)mm (mil)Typical; ASTM D3652
Total tape thickness0.046 (1.8)mm (mil)Typical; ASTM D3652
Shelf life18monthsFrom manufacture; 4 to 27 deg C and 40 to 50% RH
Technical properties

Final-state / after-processing properties

Performance values are typical; methods and conditions are shown in each row.

PropertyValueUnitMethod / condition
180 deg peel adhesion17.7 (16.2)N/100 mm (oz/in)Typical; ASTM D3330; stainless steel, 23 deg C, 72 h dwell, 304 mm/min
Tensile strength701 (40)N/100 mm (lb/in)Typical; ASTM D3759; machine direction