3M™ Scotchcast™ 260 Epoxy Powder Resin

Harmonization Code : 3907.30.20 | Epoxide resins of a kind used for coating in powder form

3M™ Scotchcast™ 260 Epoxy Powder Resin

Main features

  • Fast curing
  • Excellent electrical properties
  • Excellent flow • UL 1446 Electrical Insulation System (EIS) approval at class 120(E), 130(B), 155(F), and 180(H)

Product Description

3M™ Scotchcast™ Electrical Resin 260 is a one-part, heat-curing epoxy powder resin designed to deliver a tough, continuous dielectric coating for electrical insulation and protection. This green, pigmented resin melts, flows, and cures upon contact with preheated substrates, forming a smooth, uniform, and durable coating. Engineered through a fusion blend process, each particle contains all necessary components for complete curing and consistent performance. It is widely used for moisture-proofing and insulating electrical components in demanding environments.

Product Key Features

  • Rapid heat-curing formulation improves processing efficiency
  • Provides reliable dielectric insulation performance
  • High resistance to thermal shock, impact, and cut-through
  • Withstands heat, chemicals, and moisture exposure
  • Ensures uniform coating on flat surfaces, edges, and corners
  • Meets UL 1446 Electrical Insulation System (EIS) standards across multiple temperature classes (120E, 130B, 155F, 180H)

Applications

  • Insulating and moisture-proofing armatures and stators
  • Coating bus bars and toroidal cores
  • Electrical component protection in industrial equipment
  • Applications requiring durable dielectric coatings
  • Protective coating for components exposed to harsh environmental conditions
Product Family

3M 260

1. Select Package Type
2. Select Version
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 2 weeks
Packaging
Please select Package Type and Version.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green
Specific Gravity
1.43
Electrical Properties
Dielectric Strength
39.37 kV/mm