Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 2214

Main features

  • 82 to 177 deg C Service Range
  • One-Part Non-Sag Paste
  • Multi-Substrate High-Adhesion Bonding

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive 2214 Hi-Temp New Formula is a one-part, 100% solids, aluminum-filled epoxy adhesive designed to deliver high strength at elevated temperatures. Curing at 121°C (250°F), this deaerated, paste-consistency adhesive is specifically formulated for bonding metals and high-temperature plastics such as fiberglass-reinforced plastic, polyester, and phenolics. It is engineered to maintain robust performance in demanding environments requiring higher strengths between 82°C and 177°C (180°F to 350°F).

Key features

  • High-temperature strength: Maintains strong, reliable bonds in demanding thermal environments from 82°C to 177°C (180°F to 350°F).
  • One-part, heat-curing formula: Eliminates mixing requirements and cures thoroughly in 60 minutes at 121°C (250°F).
  • Versatile substrate bonding: Effectively adheres to metals and various high-temperature plastics, including fiberglass-reinforced plastics and phenolics[cite: 10].

Applications / Suitable for

  • Bonding metals in high-temperature environments
  • Adhering high-temperature plastics such as fiberglass-reinforced plastic, polyester, and phenolics
  • Applications requiring high structural strength between 82°C and 177°C (180°F to 350°F)
Product Family

3M 2214

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray Brown
Solids
100 %
Work life @25°C
1.1 hours
Thermal Properties
Thermal Conductivity
0.422 W/m.K
Mechanical Properties
Elongation
1 %
Peel Strength
4 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Modified Epoxy - -
Color Gray Brown - -
Net Weight 1.65 g/cm³ -
Viscosity > 1,000,000 cP Brookfield
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications

Property Value Unit Method / condition
Cured Color Gray Brown - -
Time to Full Cure 60 minutes at 121°C (250°F)[cite: 10]
Shore Hardness 85 Shore D ASTM D2240 at 23°C (73°F)
Overlap Shear Strength 17 MPa ASTM D1002, Cold Rolled Steel at 23°C
T-Peel Adhesion 9 N/cm ASTM D1876, Steel at 23°C
Thermal Conductivity 0.422 W/m/K -