3M 2158

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 2158

Main features

  • High-Strength Structural Bonding
  • 120-Minute Working Window
  • 1:1 Meter-Mix Processing

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a two-part, high-strength epoxy adhesive that chemically cures at room temperature to form a durable gray bond. It provides excellent adhesion to a wide variety of substrates, including metals, many plastics, wood, and damp concrete. Featuring a convenient 1:1 mix ratio by weight or volume, it is also recognized as meeting UL 94 HB standards for flammability.

Key features

  • Convenient mix ratio: Features a 1:1 mix ratio by weight or volume for simplified dispensing and application.
  • Versatile adhesion: Bonds strongly to multiple substrates, including metals, plastics, wood, and damp concrete.
  • Extended work life: Offers a 120-minute open time at room temperature, allowing ample time for complex assemblies and positioning.

Applications / Suitable for

  • High-strength structural bonding
  • Assembling metals, plastics, and wood
  • Applications requiring bonding to damp concrete
Product Family

3M 2158

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
1:1
Solids
100 %
Work life @25°C
2 hours
Physical Properties
Viscosity (Part A)
200,000 - 800,000 mPa.s
Viscosity (Part B)
250,000 - 450,000 mPa.s
Mechanical Properties
Elongation
54 %
Peel Strength
3 lb/in width
Electrical Properties
Volume Resistivity
1.4E+15 Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)
52 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio 1:1 - By weight or volume
Color White - Base
Color Dark Gray - Accelerator
Viscosity 250,000 - 450,000 cP Base at 23°C
Viscosity 200,000 - 800,000 cP Accelerator at 23°C
Work Life 120 minutes 100g mixed at 23°C
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Cured Color Gray - -
Durometer Hardness 85 Shore D ASTM D2240
T-Peel Adhesion 3 lb/in width ASTM D1876, FPL Etched Aluminum
Dielectric Constant 5.6 - 1 KHz (ASTM D150)
Volume Resistivity 1.4E+15 Ohm-cm ASTM D257